Molding Compounds are thermosetting plastics with very good mechanical, electrical insulation and temperature resistance properties. Depending on their chemistry, hardeners, additives, filler and filler cut size, molding compounds are destined for different applications. Epoxy molding compounds (EMC) are our main focus but there are also Bulk molding compounds and Sheet molding compounds, mainly composed by polyester or vinyl ester.

Epoxy molding compounds (EMC), known also as Epoxy resins or Duroplast are used extensively in the semiconductor, electronics and automotive industries to replace more expensive ceramics, metals and other plastics. They are mainly Silica or Fiberglass filled with various additives such as bismaleimides and anti bleeds that contribute to their thermal and mechanical properties. Krayden, being a specialised chemicals distributor, mainly focuses on industrial, automotive, optoelectronic and semiconductor epoxy molding compounds.

Please continue to our Learn More section to learn more about which epoxy molding compounds are available, the differences in their types and application methods, and how KRAYDEN can help you select and order the compound that is right for your application.

Frequently asked questions

What are the recommended dimensions of mold vents?

Mold venting dimensions depend very much on the size of the molded part. For large parts using a lot of epoxy mold compound per part, the vents are much larger than for example semiconductor molded parts. In general, on large parts, "generous" vents are recommended. This means that vent scars on larger parts are not so critical and neither is flash as long as the air is forced out.

It\'s difficult to be specific as to depth but 150 - 200 microns are figures that are typical. The wider the mold vents the better, with 5 mm or more depending on the mold layout. Double vents used to be quite common. A mold tool designer should have various rules of thumb and really is the one to decide on what is required for each epoxy mold.

Transfer molding vs. compression molding

There are two basic application methods of applying epoxy molding compound: transfer molding and compression molding.

Transfer molding means that the parts are pressed through a "cull" to a runner which then runs to the part cavities to be filled.

Compression molding, on the other hand, the bottom of the mold is the bottom of the part, and the epoxy is fed into the cavity. The top of the mold is brough down on top, forming the top of the part.

What is an Acetone test for EMC?

We regularly test our EMC for agglomerate particles. While a very rare occurrence, it can happen so we have quality testing in place. An acetone test, otherwise known as hard spot test, is a standard test method employed by our QC Dept. to detect and capture agglomerate in mold compoundS.

The test starts by putting the mold compound in acetone. Organic components will dissolve in it while inorganic components (mainly silica filler) and agglomerate particles will remain undissolved. By running the solution through a combination of sieves with different mesh sizes we are able to catch any agglomerate particles in the sieve and determine whether the EMC was contaminated or not.

Wouldn\'t electrically conductive fillers provide better thermal conductivity?

Yes, they would. However, there is an implicit understanding when epoxy mold compound manufacturers refer to "thermally conductive" EMCs. What they are actually saying is "thermally conductive and yet still electrically insulating".

The reason is because functional epoxy mold compounds used for semiconductor encapsulation have a first, basic function - and that is to electrically insulate. Once this basic need is provided, we can look at providing thermal conductivity, which rules out electrically conductive fillers.

What is the highest Tg possible for an EMC?

Base epoxies probably have a current maximum Tg of around 255°C. When combined with other resins, hardeners and polymers, we have seen thermosetting polymers with a Tg as high as 454°C, though this material is not designed for semiconductor encapsulation.

Can Epoxy Mold Compounds be used in applications that are above their Tg?

Absolutely. An epoxy\'s glass transition temperature is not the same as its maximum operating temperature. Some materials, such as silicones have glass transition temperatures that rare low, or even negative and yet can have maximum operating temperatures higher than epoxies.

What is the best material to use for high thermal conductivity in Epoxy Mold Compounds?

If price was not a concern, diamond would be the best thermally conductive filler to use. It has a bulk thermal conductivity of 2200 W/mK and mixes well with epoxy resins to offer excellent flow properties.

Furthermore, it is an excellent electrical insulator. Unfortunately, the price for such a compound would be upwards of $7500/kg which makes it far too expensive for practical applications.

When the filler density and the crosslink density of different resins are different, in which way it affects the resin properties?

For filler density, specifically, the use of silica fillers has the following impacts on molding compound properties: 

  • Reduced: Shrinkage (thus, thermal stress), CTE & Water Absorption, formulation cost, exothermic property
  • Improved: toughness & abrasion resistance & Thermal conductivity, heat deflection temperature, modulus
  • Increased: Viscosity & Weight & Dielectric Constant & Matching Difficulties

 

Molding Compound Categories
Application Key Properties
Attributes Main Colors Filler Type Cure Chemistry Glass Transition
Temperature (Tg), °C
CTE, Alpha 1
ppm/°C
CTE, Alpha 2
ppm/°C
Industrial Thermal shock and mechanical resistance Black Fiberglass Anhydride 105 - 161 17 - 42 50 - 118
Semiconductor Fine filled and Electrically stable Black, Gold Silica Phenolics 162 - 191 18 - 21 60 - 70
Optoelectronics Highly reflective and transmissive White, Clear Proprietary Hybrid 137 - 151  41 - 81 90 - 167

*All properties are indicative. There are other colors/cure chemistries and filler types for each category but the table points out the main application characteristics.

 

 

Pellet Diameter Capability
  Pellet Diameter Pellet Weight Range (grams)
Type Millimeters Inches Minimum Maximum
Micro Pellets 5 0.197 0.2 0.4
  5.7 0.224 0.35 0.55
  8.5 0.335 0.8 1.2
Mini Pellets 11 0.433 1.5 4.5
  13 0.512 2 6
  14 0.551 2.5 7.5
  14.3 0.563 2.5 8.5
  16 0.63 3.5 12
  18 0.709 4 16
  20 0.787 5 20
  25 0.984 8 30
Conventional Pellets 35 1.375 20 70
  38 1.496 25 85
  40.6 1.6 20 160
  45 1.75 35 120
  48 1.9 40 135
  55 2.165 50 180
  58 2.28 40 380
  61 2.4 45 400

 


Learn more

Epoxy Mold Compounds (EMC) are formulations of thermosetting solid epoxy polymers, additives, and silica-based fillers.

EMCs are used in industrial molding applications and commonly come in the form of compressed solid powder pellets which are then heated into a liquid and molded to encapsulate or “package” a semiconductor or electronic device.

The final mold form of Thermosets is permanent

They won’t melt again even at higher temperatures than their original melting point. This makes them perfect for high-temperature applications including circuit board devices which have to go through a solder reflow process of up to 260°C.

Epoxy Mold Compounds are composites of epoxy resin(s), filler(s) and additives. They are solid pellets of powder that are heated into a liquid and then permanently set into their molded shape in a thermosetting process

Epoxy is produced by combining epichlorohydrin with a Curative (hardener).

The most common curatives are Bisphenol-A (DGEBA), Bisphenol-F (DGEBF). However, other curatives are also used: including Phenols, Thiols, Anhydrides, Amines, Aliphatic Alcohols. Depending on the curative and the ratio of curative to epichlorohydrin the resulting resins can have a variety of molecular weights, viscosity, and final material properties.

The final result is usually a complex crosslinked long-chain molecule polymer network with great strength, and high thermal and chemical resistance, fast cure time, and low viscosity. Combining it with a silica filler dramatically lowers CTE, increases density, and creates a mechanically strong and incredibly insulating composite perfect for insulating and protecting even the most sensitive electric devices.

 

Hardeners and Curatives.

Different curatives produce different kinds of epoxy resins with different properties. For example, Bisphenol epoxy resins are most commonly used as a base for adhesives and coatings. Epoxy Mold Compounds (EMC) on the other hand are usually a formulation of either anhydride epoxy resin or phenolic epoxy resins, along with other additives, and including a high percentage silica-based filler (60%--90%).

Epoxy resins cured with anhydrides have low viscosity, high latency, and have amazing cured strength

This makes them perfect for Industrial EMC for molding larger and more massive parts that require higher mechanical strength. However, anhydride epoxies generally have high moisture absorption which makes them less suited to more sensitive electrical applications like semiconductors.

Phenol curatives form highly crosslinked polymer networks: and so have outstanding high temperature and chemical resistance and lower moisture absorption.

That's why phenolic epoxy resins are perfect in Semiconductor Epoxy Mold Compounds because they can easily survive even SAC solder reflow temperatures (260 °C). This makes phenolic epoxy resin based EMC the standard for semiconductor encapsulation and other high-temperature applications.

 

Fillers

Different filler types also dramatically affect the final properties of the resulting EMC composite. For example, adding iron filler creates EMC with higher thermal conductivity and other magnetic properties, whereas silica filler increases the strength and insulation of the final composite.

One important reason silica fillers are the most used mineral filler in EMC composites is that silica has an incredibly low coefficient of thermal expansion (CTE).

Epoxy resin by itself has a CTE of 300ppm/°C, while silica has a CTE of 3ppm/°C

Combining the two creates a final composite with a CTE of around 60ppm/°C in a ratio of 80% filler to 20% epoxy resin.

Having a low CTE EMC is important to ensure that the Epoxy Mold Compound packet and the semiconductor or electric device inside expand and contract at the same rate under thermal stress otherwise delamination will occur.

There are two main types  of Silica-based filler pure Si02 silica sand and fiberglass which is a Si02 based glass fiber

Silica filler comes in two main types: Fibreglass and silica sand.

Fiberglass, like all glass, is silica based and generally has a higher particle size. Fiberglass fibers create an interlocking structure giving increased mechanical strength, however, it has a much larger particle size and higher viscosity because fiber is unable to flow very well in the molten composite.

Not just the filler type, but filler particle size and ratio have an important impact on the final performance of any given EMC.

Silica sand, on the other hand, has a smaller particle size, and particles that are more spherical and so flow better when the composite is molten. Smaller gate size 100 microns, a general rule filler particle size needs to be less than 1/3 the gate size.

Filler particle size may be the most important variable when it comes to selecting an Epoxy Mold Compound

In the EMC molding process, the solid epoxy molding compound is heated to become a liquid and then must flow through runners and gates of the mold plate that direct it into the mold cavity. Transfer molding plates for semiconductors can have gate sizes as small as 100 microns. Fiberglass filler can have particle sizes of 100 microns so are clearly incompatible. Silica Sand can have particle sizes of less than a micro making it the perfect choice for semiconductor encapsulation.

 

Industrial EMC vs. Semiconductor EMC

Epoxy molding compounds (EMCs) are the workhorses of modern encapsulation but not all EMCs are created equal. Broadly, they fall into two main families, each tailored to a very different operating environment.

Industrial EMC

Industrial EMCs are typically formulated from anhydride-cured epoxy resins reinforced with fiberglass. This combination produces a rigid composite with high mechanical strength, thermal stability, and electrical insulation, making it ideal for larger and more robust molded parts. Glass-filled epoxy systems offer:

  • High mechanical and dimensional stability: greater stiffness/strength and creep/fatigue resistance, holding tight tolerances under load and thermal cycling.
  • Durable electrical insulation: high dielectric/arc resistance, low moisture uptake, and reliable adhesion for sealed, long-life assemblies.

 Typical Use Cases

  • Power and high-voltage insulation: primary bushings, switchgear insulators, and terminal blocks
  • Automotive and transportation: molded solenoids, ignition and engine control units, sensors, and connector housings
  • Industrial automation: coil housings, relays, and encapsulated transformers

These applications require dimensional rigidity, impact resistance, and outdoor reliability areas where fiberglass-filled, anhydride-cured systems excel.

Semiconductor EMC

Semiconductor EMCs, by contrast, use phenolic-cured epoxy resins filled with fine silica (SiO₂).

The micron-sized silica particles provide excellent flow through narrow transfer-molding gates, enabling complete, void-free encapsulation of tiny semiconductor components. More importantly, phenolic epoxy systems offer:

  • Superior thermal and chemical resistance: withstand solder reflow and high-temperature reliability tests
  • Lower moisture absorption: prevent delamination and corrosion
  • Low ionic and dielectric properties: ensure electrical stability and long device life

Typical Use Cases

  • Integrated circuits (ICs): SOIC, QFP, BGA, and power IC packaging
  • Optoelectronics: IRDA sensors, LED encapsulation, photodiodes
  • Automotive electronics: engine control units (ECUs), power modules, and sensors

These materials prioritize precision, purity, and reliability over brute strength protecting the most sensitive components in modern electronics.

Industrial Epoxy Mold Compound and Semiconductor Epoxy Mold Compound have been forrmulated for different applications

Key Properties

Moisture Absorption

EMC Semiconductors have to meet much higher requirements formalized in the industry as MSL standards. Moisture absorption is one the most important factors: trapped moisture within the epoxy molding compound expands explosively as steam and literally cause the encapsulated semiconductor to explode like a popcorn. 

That's why depending on epoxy resin type and silica filler type, epoxy mold compounds are suited for either industrial product molding or semiconductor molding.

Glass Transition Temperature (Tg)

As explained in the article on how epoxy mold compounds cure, the glass transition temperature (Tg) of an epoxy molding compound is the temperature above which epoxy properties, specifically the coefficient of thermal expansion (CTE) and the dynamic modulus (E), change.

As you can see in Figure 1, the glass transition temperature, though often presented on technical data sheets as a single value is actually more accurately defined as a range. On the left side of the range, the epoxy mold compounds exhibit a hard or glassy behavior, characterized by a high modulus, high hardness and high stiffness. On the right side of the glass transition temperature the epoxy mold compound has a lower modulus, lower hardness and lower stiffness.

Similarly, the lower line represents the dimension or volume of the EMC. On the left of the glass transition region, the coefficient of thermal expansion (CTE), measured in parts per million per degree Celcius (or ppm/°C) is linear and its rate ofd expansion increases more slowly. On the right side of the Tg region, the CTE increases much more quickly, typically 3 to 4 times as much in the case of epoxy molding compounds.

Epoxy Mold Compound Properties affected by Glass Transition TemperatureFigure 1. Epoxy Mold Compound Properties affected by Glass Transition Temperature (Tg)
Comparative Tracking Index

As the progress of semiconductor packages continuously moves towards high voltage, high power, and high frequency, insulation becomes nonnegotiable. Comparative Tracking Index (CTI) measures a material’s resistance to electrical tracking—the formation of a conductive carbonized path on the surface of an insulator under moisture and voltage stress.

Tracking Index (V) Material Group PLC
600 and Greater I 0
400 through 599 II 1
250 through 399 III 2
175 through 249 IIIa 3
100 through 174 IIIb 4
< 100 - 5

Comparative Tracking Index (CTI) test determines the maximum voltage at which the material resists tracking after 50 drops of 0.1 % ammonium chloride solution have fallen between two electrodes placed on the surface of a 3 mm thick specimen. 

CTI result is expressed in volts and categorized into Performance Level Categories (PLC) and Material Group to standardize material classification. 

A high CTI value indicates strong resistance to surface leakage and tracking, allowing reduced creepage distances and safer design in high-voltage or humid environments. Epoxy molding compounds with CTI ≥ 600 V (PLC 0) are ideal for power modules, relays, automotive control units, and high-reliability semiconductor packages. Conversely, materials with CTI < 250 V (PLC ≥ 3) require greater creepage distances or environmental protection to prevent arcing and insulation failure.


EMC Electrical Properties

Understanding what the numbers mean and when they matter

Electrical properties are frequently requested when reviewing epoxy molding compounds, or EMCs, but the value alone is rarely enough. A number that looks strong on a datasheet can still be misleading if the test method, specimen condition, frequency, temperature, humidity, thickness, applied voltage, or electrode geometry do not match the actual application.

The table below summarizes the core electrical properties commonly discussed for EMCs, what each property measures, why it matters, how to interpret it, and what conditions most strongly affect the result. For meaningful comparison, always review the property together with the test method and the application context rather than treating the number as a standalone rating.

Property What it measures Why it matters Typical example range How to interpret it Key condition sensitivities / notes Primary scope
Dielectric strength Maximum electric field before electrical breakdown, often reported as breakdown voltage normalized by thickness. Defines short-term insulation margin and is important for high-voltage and tight-spacing designs. ~15 to 30 kV/mm Higher is generally better, but it indicates breakdown limit, not operating leakage or long-term insulation reliability. Strongly affected by thickness, electrode geometry, surrounding medium, ramp rate, and test method. Material / package
Dielectric constant (Dk) Relative permittivity, or the ability of the EMC to store electric energy in an electric field. Influences parasitic capacitance, signal behavior, and electric field distribution inside the package. ~3.5 to 5.0 at 1 MHz Lower is often preferred, but the right value is application-dependent and should not be reviewed alone. Must be read together with frequency, temperature, moisture condition, and dissipation factor. Material / package / system
Dissipation factor (Df, tan δ) Fraction of electrical energy lost as heat under AC fields. Controls dielectric loss and heating, especially in AC, switching, and high-frequency applications. ~0.005 to 0.03 at 1 MHz Lower is better. Usually increases with frequency, temperature, and moisture, so test conditions must be known. Material / package / system
Volume resistivity Resistance to current leakage through the bulk material. Indicates bulk insulation capability and supports discussions of bulk leakage under bias, but does not replace structure‑level M&IR data. ~1014 to 1016 Ω·cm (dry) Higher is better. Can drop significantly with moisture, ionic contamination, elevated temperature, and differences in specimen geometry or electrode setup. Material / package
Surface resistivity Resistance to leakage current along the material surface. Critical under humidity, contamination, and residue exposure, where surface leakage can dominate failures. ~1013 to 1016 Ω/sq (dry) Higher is better. Extremely sensitive to moisture, cleanliness, residues, contamination, and environmental conditioning. Material / package / system
Insulation resistance / M&IR Leakage resistance of an insulated structure under voltage. M&IR includes moisture exposure. Often the most application-relevant insulation metric because it reflects real electrical behavior under bias. Dry: >1012 to 1013 Ω, but values can drop by orders of magnitude after humidity exposure Higher is better. Depends strongly on test standard, bias, humidity, temperature, duration, leakage-current definition, and structure design. Package / system
CTI Maximum standardized voltage resisting surface tracking under contaminated conditions. Used for creepage design, pollution exposure review, and material grouping. ~175 to ≥600 V Higher is better. CTI is a surface tracking property. It should not be confused with bulk breakdown, bulk leakage, or general insulation reliability. Material / package / system
Arc resistance Resistance of the surface to degradation from electrical arcing. Relevant where intermittent discharge or arcing may occur. ~60 to 180+ seconds Higher is better. Surface formulation and filler system strongly affect the result. It is unrelated to dielectric constant or dielectric strength. Material / package / system
DWV / HiPot Ability of a defined structure to withstand a specified voltage for a set time. Used for production screening and qualification requirements. Application-specific, pass/fail It is pass/fail, not a graded material rating. Strongly dependent on package geometry, insulation path, voids, contamination, defects, and full assembly design. Passing does not prove long-term reliability. Package / system

In practice, the right question is not only what the value is, but how it was measured, under what conditions, and whether that matches the application. When that context is clear, EMC electrical data becomes much more useful for material selection, customer discussion, and reliability review.

 


Product Handling Guide

Protection from Heat & Humidity

Epoxy Molding Compounds (EMC) are affected by heat and moisture. That is why we require refrigeration during shipping, handling, and storage.

Heat (above suggested storage condition) will cause the epoxy molding compound to slowly begin to react, reducing the material’s spiral flow length and gel time. This may lead to product process variations that may be required to mold successfully.
Condensation or high humidity (>50%) may cause the epoxy to cure more slowly, which in turn may reduce the material’s viscosity. This may lead to mold defects and could also reduce material properties.
 

Epoxy Mold Compounds are shipped in plastic bags packed in carton boxes. The plastic bags keep the condensation and humidity from coming into contact with EMC and should only be opened and closed when the epoxy is at room temperature to avoid condensation formation when moving the products from cold storage to warmer temperatures.

Upon recieving the products, move the products into cold storage. When you receive your goods, they should be placed into cold storage as soon as possible. KRAYDEN recommends materials be stored at or below the storage temperatures indicated on the technical data sheets. Lower temperatures are even better to maximize flow retention.MaximizingFlowRetention

Storage Instructions

Store Epoxy Molding Compound (EMC) as cool as possible. Epoxy molding compounds are mixed systems wherein the cross-linking reaction is initiated at the time of manufacturing. This reaction causes the flow retention to drop, meaning it flows less during molding. Once started, the reaction cannot be stopped, only slowed down. This rate of reaction is dependent on two factors: time and temperature

EpoxyMoldingCompoundFlowRetentionRate

Storing epoxy molding compounds at lower temperatures slows down the reaction significantly. Though the rate of reaction is different for every product, the chart below gives a good idea of what happens to mold compound flow retention at various storage temperatures. Though KRAYDEN typically recommends a storage temperature at or below the temperature listed on the technical data sheet, you can see from below chart that lower temperatures have an even more positive on flow retention rates.

 

Usage Instructions

  1. Remove Epoxy Molding Compound from cold storage. Epoxy Molding Compounds must be brought to ambient temperature before use. The time for temperature equilibration depends on the mass of material being prepared for use. A 15kg box of EMC stored at 5°C needs approximately 4 hours to equilibrate. Boxes stored at colder temperatures need longer times. KRAYDEN typically recommends taking EMC from cold storage 8 – 24 hours before use. Use product within 48 hours.
  2. Do NOT open plastic bag before thawing. Condensation may form on the box and the bag of the EMC when brought to temperature to equilibrate. This is normal and poses no problems. If the bag is opened, condensation may form on the pellets, this may cause molding issues. Keep the bag closed until ready for use.
  3. Do NOT return unused product to cool storage. It is not advised for unused product to be returned to cold storage. Though it is possible to refreeze and re-thaw the EMC, it is very difficult to measure the remaining flow retention and thus, KRAYDEN voids all warranties in these cases. If you do choose to do this, make sure the plastic bags is well sealed prior to returning to cold storage to avoid condensation.

Reliability and Standards

In JEDEC-style qualification, epoxy molding compound reliability is primarily governed by moisture, thermo-mechanical mismatch, ionic cleanliness, and interface durability. A typical flow is Moisture Preconditioning → Pb-free Reflow, then the remaining stresses are commonly executed in parallel to isolate dominant failure modes.

Important clarity: JEDEC/IPC methods define test conditions and pass/fail criteria. The “mechanism, sensitivity, and FA focus” notes below are engineering interpretation based on widely reported package reliability behavior (not JEDEC-prescribed rankings or guaranteed signatures).

Qualification stress (standard) What the method is intended to stress (per standard) Common FA observations to monitor  EMC evaluation focus 
Moisture Preconditioning
JESD22-A113
Standardized moisture exposure / soak used to condition parts prior to downstream stresses (e.g., reflow and humidity/bias tests).
IR drop while wet; early interface weakening indicators; baseline CSAM snapshot for later comparisons.
Moisture plasticization reduces modulus and can depress effective Tg, lowering mechanical margins during reflow or cycling
Insulation resistance / resistivity can drop while wet (reversible if no damage)
Moisture can increase ion mobility of existing residues (not “creating” new ions)
(Note: JEDEC does not define “ionic contamination limits” for plastic packages; ionic cleanliness is an industry-driven risk-screening metric.)
Pb-free Reflow / MSL-Reflow Exposure
IPC/JEDEC J-STD-020
Solder reflow temperature-time exposure (and MSL classification framework) to evaluate moisture-sensitivity risk and assembly survivability.
CSAM for die paddle / leadframe delamination; “popcorn” cracking where applicable.
Cross-sections at known stress concentrators (die corners, paddle edges).
Vapor-pressure + above-Tg mismatch strain can drive delamination/cracking in moisture-loaded packages
Interface durability (Cu/die paddle) becomes the dominant package-level limiter in many designs
Microvoids / microcracks (if present) can amplify subsequent moisture ingress sensitivity
Thermal Cycling
JESD22-A104
Repeated temperature excursions to accelerate thermo-mechanical fatigue of the package and interconnect structures.
CSAM delamination growth trend vs cycles.
Microcrack mapping in high-stress regions; warpage/strain correlation where available.
CTE mismatch fatigue can progressively degrade interface integrity
CTE behavior below/above Tg (the “Tg-jump”) influences stress amplitude
Interfacial toughness (not just “adhesion strength”) helps suppress delam growth
uHAST / Unbiased Temperature-Humidity
JESD22-A118
Accelerated moisture/temperature exposure without applied electrical bias to evaluate humidity robustness (unbiased condition).
CSAM delamination checks.
Electrical IR recovery behavior after bake-out (damage-dependent); interface-focused cross-sections when anomalies persist.
Hot moisture ingress can drive wet-state IR/resistivity reduction
Interface durability under hot/wet conditions (delamination risk)
Note: At uHAST temperatures (e.g., 130 °C), many EMCs may be at/above (wet) Tg, which 
can be significantly lower than dry Tg, accelerating mechanical compliance changes during uHAST.
HAST / BHAST
JESD22-A110
Accelerated moisture/temperature exposure with electrical bias to evaluate susceptibility to humidity + bias driven degradation (leakage, corrosion, parametric drift).
Leakage trend vs time.
Corrosion and ion-migration evidence (where applicable); dendritic bridging.
Delamination localized to corrosion-affected regions.
Leakage / IR collapse risk-screening is strongly influenced by moisture + field + contamination state
Ionic cleanliness (industry metric) can be a major differentiator for pass likelihood
Cu/metal interface degradation can occur in some stacks when corrosion chemistry and interface conditions align (finish, promoters, residues)
THB / 85-85 High-V Bias
JESD22-A101
Temperature-humidity-bias exposure (often long duration) to evaluate humidity + electrical bias robustness under 85/85 class conditions.
Dendritic shorts/bridging; leakage runaway.
Surface/bulk conduction path localization and contamination mapping.
Ionic cleanliness + moisture uptake/diffusivity govern conductive path formation risk
Resistivity retention under humidity + field is the practical discriminator
(Note: JEDEC does not prescribe ionic contamination limits for plastic packages; “ionic cleanliness” is commonly monitored via industry analytical methods.)
HTRB / High Temperature Reverse Bias
JESD22-A108
Device-level temperature + bias stress intended to accelerate electrically/thermally activated wear-out and parametric drift under reverse-bias conditions.
Electrical drift/fail signatures.
Post-stress CSAM for any delamination growth (package-dependent).
Brittleness/crack propensity checks if the program includes post-HTRB mechanical/thermal follow-on.
Packaging effects are typically secondary vs device/interconnect physics
For EMC, the key question is Tg margin and high-temperature stability of mechanical/adhesion properties at 150–175 °C
Long exposure can increase brittleness risk in some systems (case- and chemistry-dependent)
Note: HTRB is historically device/interconnect dominated; EMC aging effects are usually secondary unless Tg is marginal for the stress temperature.

Note: This table is structured for qualification planning readability. JEDEC/IPC method names indicate the test procedure; the “sensitivity themes” and “FA focus” columns reflect common engineering interpretation, not JEDEC-defined rankings.

What this means for selecting an EMC 
The priorities below reflect common engineering selection logic used to improve pass likelihood in specific stress families. They are not prescribed by JEDEC, but align with broadly reported package reliability behaviors.
Popcorn / delamination risk
Prioritize low moisture uptake plus strong Cu/die-pad adhesion durability through preconditioning + Pb-free reflow.
Leakage / corrosion under humid bias
Prioritize ultra-low ionic content and resistivity retention under moisture + electric field (HAST / THB).
Cycle fatigue (temperature cycling)
Prioritize CTE behavior (below/above Tg) and interfacial toughness to suppress progressive delamination in TC.
High-temperature exposure (HTRB)
Prioritize thermal robustness at 150–175 °C and toughness retention to reduce brittle cracking propensity and packaging-side risk when Tg margin is tight.

Thermal Role of Epoxy Molding Compounds in Power Packages

Epoxy molding compounds (EMCs) in power packages do more than provide mechanical protection and environmental sealing, they also participate in the heat flow from the semiconductor junction to the outside world. In leadframe-based power packages (DPAK/D²PAK, TO-220/247, power QFN, SOP/QFP), most heat still leaves the die through the die-attach and leadframe into the encapsulant, PCB, or heatsink (primary junction-to-encapsulant path) However, once the die is encapsulated, the EMC forms a parallel conduction path around and above the chip, feeding heat into the mold cap, leads, and surrounding air or heatsink surfaces and therefore influencing both junction-to-encapsulant and junction-to-ambient resistances. In compact surface-mount power packages with a large mold volume and limited exposed metal, the relative contribution of the EMC path increases, so its thermal properties become critical for keeping junction temperatures within design limits.

 
The thermal conductivity k of the molding compound directly affects package-level thermal resistance, r_th, by changing how efficiently the mold body can spread and conduct heat away from the die. Standard silica-filled EMCs typically have k ≈ 0.6–0.9 W/m·K, which is far higher than air but much lower than copper or ceramic, making the compound a “bottleneck” once heat reaches the encapsulant. By increasing k via high-thermal fillers (e.g., alumina, AlN, BN, Si₃N₄) at high loading, EMCs with k in the 2–5 W/m·K range are possible; mixture models such as Bruggeman’s law describe how composite k rises with filler volume fraction. Package-level measurements on QFP and SOP power packages show that moving from a general-purpose EMC (k ~1 W/m·K) to a high-thermal EMC (k ≥3 W/m·K) can reduce total thermal resistance by on the order of tens of percent, with stronger benefits under natural convection and for packages where the mold cap represents a large portion of the heat-flow cross-section. In practice, the EMC’s k is therefore a key design knob for tuning junction-to-encapsulant path and junction-to-ambient path in power packages, balanced against typical trade-offs in flow, viscosity, stress, and reliability that come with high filler loading.

Presentations

Introduction to Mold Compound

A quick overview on what mold compounds are along with its properties and relevant applications. 

Properties and Characterization

Properties of Epoxy Molding Compounds and the characterization processes involved. 

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers