3M 1099
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Medium-Viscosity Application Control
- Long-Term Durability by Resisting Weathering
- Adhesion-Promoting Surface Treatment
Product Description
3M™ Nitrile High Performance Plastic Adhesive 1099 is a fast-drying, medium-viscosity nitrile rubber adhesive designed for brush or flow applications. It cures to form strong, flexible bonds that resist weathering, water, fuels, oil, and plasticizers. This high-performance adhesive can be used at room temperature or heat-cured to obtain superior physical properties, making it highly versatile for various assembly needs.
Key features
- Fast drying: Rapidly forms strong, flexible bonds to help accelerate production and assembly processes.
- Exceptional resistance: Delivers robust durability against weathering, water, fuels, oil, and plasticizers.
- Heat-cure option: May be cured with heat to achieve superior physical and mechanical properties.
Applications / Suitable for
- Bonding vinyl extrusions and sheeting
- Adhering fabrics, foams, and many plastics
- Industrial brush or flow applications
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base | Nitrile Rubber | - | - |
| Color | Light Tan | - | Wet and dry |
| Solids Content by Weight | 31-37 | % | - |
| Carrier Solvent | Acetone | - | - |
| Viscosity | 2000-4000 | cP | at 27°C (80°F) |
| Flash Point | -15 | °C | Closed Cup |
| Bonding Range | Up to 40 | minutes | - |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180° Peel Adhesion | 29 | N/cm | Canvas to Steel, 24h at 23°C (73°F) |
| 45 | N/cm | Canvas to Steel, 72 h at 23°C (73°F) | |
| 48 | N/cm | Canvas to Steel, 168 h at 23°C (73°F) | |
| 54 | N/cm | Canvas to Steel, 14 days at 23°C (73°F) | |
| 31 | N/cm | Canvas to Steel, 21 days at -34°C (29°F) | |
| 12 | N/cm | Canvas to Steel, 21 days at 66°C (150°F) | |
| Overlap Shear Strength |
3.2 | MPa | Aluminum to Aluminum, 121°C cure |
| 21 | MPa | Aluminum to Aluminum, 177°C cure, tested at -55°C | |
| 9.0 | MPa | Aluminum to Aluminum, 177°C cure, tested at 23°C | |
| 6.2 | MPa | Aluminum to Aluminum, 177°C cure, tested at 66°C |