3M 1205
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 155 deg C Continuous Operation
- 6000 V Dielectric Minimum
- Coil and Solder-Mask Versatility
Product Description
3M Polyimide Film Electrical Tape 1205 is an amber, 0.081 mm polyimide tape with a non-corrosive acrylic pressure-sensitive adhesive for electrical insulation and solder masking. Its 0.025 mm film backing provides a thin insulating construction for coils, capacitors, transformers, wire harnesses, lead anchoring, and printed circuit board assembly. The tape is designed for continuous operation not exceeding 155 deg C under its UL listing. ASTM D1000 values include minimum dielectric breakdown of 6000 V, minimum insulation resistance of 1 x 10^12 ohm, and minimum elongation of 50%, with properties measured at 23 deg C unless otherwise stated.
Key features
- 155 deg C operation: The tape is designed for continuous operation not exceeding 155 deg C under its UL listing.
- 6000 V dielectric minimum: ASTM D1000 dielectric breakdown is at least 6000 V at 23 deg C.
- Pressure-sensitive installation: The acrylic adhesive requires no heat, moisture, or solvent preparation for application.
Applications
Applications include wrapping coils, capacitors, transformers, and wire harnesses; anchoring leads; and solder masking during printed circuit board assembly.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Amber | - | Visual |
| Backing | Polyimide film | - | As supplied |
| Adhesive | Acrylic | - | Non-corrosive pressure-sensitive adhesive |
| Backing thickness | 1 / 0.025 | mil / mm | Nominal |
| Total thickness | 3.2 +/- 0.5 / 0.081 +/- 0.013 | mil / mm | ASTM D1000 at 23 deg C |
| Shelf life | 5 | years | From manufacture; 10 to 27 deg C and less than 75% RH |
Final-state / after-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Continuous operating temperature | 155 | deg C | Maximum under UL listing |
| Dielectric breakdown | 6000 | V | Minimum; ASTM D1000 at 23 deg C |
| Insulation resistance | 1 x 10^12 | ohm | Minimum; ASTM D1000 at 23 deg C |
| Electrolytic corrosion factor | 1.0 | - | 3M ETM-54001; 1.0 equals no observed corrosion |
| Adhesion to steel | 20 / 2.2 | oz/in / N/cm | Minimum; ASTM D1000 at 23 deg C |
| Breaking strength | 20 / 35 | lb/in / N/cm | Minimum; ASTM D1000 at 23 deg C |
| Elongation | 50 | % | Minimum; ASTM D1000 at 23 deg C |
| Flame retardancy | Pass | - | UL 510A |