3M 2084
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- One-Part No-Mix Application
- Five-Minute Tack-Free Time
- Flexible Fluid-Resistant Seal
Product Description
3M Scotch-Seal Metal Sealant 2084 is a one-part, aluminum-colored, medium-viscosity sealant for bonding and sealing aluminum to glass, other metals, and wood. The acetone-based material applies without mixing and air dries to a tough, flexible film that resists water, oil, and fuel. Typical tack-free time is 5 minutes, with approximately 24 hours to dry and gap-filling capability to 1/16 in. The cured sealant retains internal integrity and can be painted after skinning; painting after cure is recommended for areas exposed to ultraviolet light. It supports general industrial sealing, metalworking, and aluminum-to-glass assembly where a flexible fluid-resistant seal is required.
Key features
- One-part application: The medium-viscosity sealant dispenses without mixing and air dries after placement.
- Five-minute tack-free time: The applied material reaches a typical tack-free condition in approximately 5 minutes.
- Flexible fluid resistance: The dried film resists water, oil, and fuel while retaining sealing integrity.
Applications
Applications include general industrial sealing, metalworking, sealing metal joints and seams, and bonding or sealing aluminum to glass, other metals, and wood.
TDS, SDS & Technical Documents
Technical Specifications
Physical Properties
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Aluminum | - | Typical |
| Viscosity | 7,000 to 22,500 | cP | Approximate; Brookfield RVF #6 at 20 rpm and 26.7 deg C |
| Solids content by weight | 40 to 47 | % | Approximate |
| Weight per gallon | 7.7 to 8.1 | lb/gal | Approximate |
| Flash point | 0 (-18) | deg F (deg C) | Closed cup |
| Coverage | 1,500 | lineal ft/gal | 1/8 in diameter wet bead |
Final-state / after-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Tack-free time | 5 | min | Approximate |
| Dry time | 24 | h | Approximate |
| Gap-filling capability | 1/16 | in | Typical |
| 180 deg peel adhesion | 25 | lb/in width | Canvas to aluminum; 2 in/min pull rate |