3M 2214
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 82 to 177 deg C Service Range
- One-Part Non-Sag Paste
- Multi-Substrate High-Adhesion Bonding
Product Description
3M™ Scotch-Weld™ Epoxy Adhesive 2214 Hi-Temp New Formula is a one-part, 100% solids, aluminum-filled epoxy adhesive designed to deliver high strength at elevated temperatures. Curing at 121°C (250°F), this deaerated, paste-consistency adhesive is specifically formulated for bonding metals and high-temperature plastics such as fiberglass-reinforced plastic, polyester, and phenolics. It is engineered to maintain robust performance in demanding environments requiring higher strengths between 82°C and 177°C (180°F to 350°F).
Key features
- High-temperature strength: Maintains strong, reliable bonds in demanding thermal environments from 82°C to 177°C (180°F to 350°F).
- One-part, heat-curing formula: Eliminates mixing requirements and cures thoroughly in 60 minutes at 121°C (250°F).
- Versatile substrate bonding: Effectively adheres to metals and various high-temperature plastics, including fiberglass-reinforced plastics and phenolics[cite: 10].
Applications / Suitable for
- Bonding metals in high-temperature environments
- Adhering high-temperature plastics such as fiberglass-reinforced plastic, polyester, and phenolics
- Applications requiring high structural strength between 82°C and 177°C (180°F to 350°F)
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base | Modified Epoxy | - | - |
| Color | Gray Brown | - | - |
| Net Weight | 1.65 | g/cm³ | - |
| Viscosity | > 1,000,000 | cP | Brookfield |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Cured Color | Gray Brown | - | - |
| Time to Full Cure | 60 | minutes | at 121°C (250°F)[cite: 10] |
| Shore Hardness | 85 | Shore D | ASTM D2240 at 23°C (73°F) |
| Overlap Shear Strength | 17 | MPa | ASTM D1002, Cold Rolled Steel at 23°C |
| T-Peel Adhesion | 9 | N/cm | ASTM D1876, Steel at 23°C |
| Thermal Conductivity | 0.422 | W/m/K | - |