3M 231/231A

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M 231/231A

Main features

  • Instant-Adhesion Paint Masking
  • Clean Multiple-Bake Removal
  • Conformable Mini-Crepe Backing

Product Description

3M Paint Masking Tape 231/231A is a tan, smooth mini-crepe paper tape for industrial and aerospace paint masking, including multiple-bake finishing operations. Its rubber adhesive provides instant adhesion and holding power, while the heat-resistant, solvent- and moisture-resistant backing conforms around complex shapes and tears cleanly for efficient application. Typical construction values include 0.19 mm total thickness, 10% elongation at break, and 49 N/cm tensile strength. The tape provides clean removal following a 30-minute exposure at temperatures up to 149 deg C under the stated condition and is suited to painting automobiles, aircraft, trucks, boats, and fabricated parts. Best results are obtained when it is applied and removed within 24 hours.

Key features

  • Instant paint-mask adhesion: The rubber adhesive sticks quickly and resists lifting or curling during supported finishing work.
  • Multiple-bake clean removal: The tape removes cleanly after 30 minutes at temperatures up to 149 deg C under the stated condition.
  • Conformable mini-crepe backing: The smooth backing follows complex shapes, resists bleed-through, and tears cleanly.

Applications

Applications include industrial paint masking, aerospace masking, multiple-bake finishing, and painting automobiles, aircraft, trucks, boats, and fabricated parts.

Product Family

3M 231/231A

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
rubber
Color Color
Tan
Total Thickness Total Thickness
190 μm
Mechanical Properties
Adhesion Strength Adhesion Strength
30.2 Oz/in
Elongation Elongation
10 %

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
ColorTan-Typical
BackingSmooth mini-crepe paper-Heat-resistant saturant
AdhesiveRubber-Typical
Total thickness0.19 (7.6)mm (mil)ASTM D3652
Elongation at break10%ASTM D3759
Tensile strength49 (28)N/cm (lb/in)ASTM D3759
Technical properties

Final-state / after-processing properties

PropertyValueUnitMethod / condition
180 deg peel adhesion4.1 (38)N/cm (oz/in)ASTM D3330 at 23 deg C; 304 mm/min
Clean-removal bake resistanceUp to 149 (300)deg C (deg F)30 min
Recommended indoor exposureApply and remove within 24hBest-results condition
Backing resistanceSolvent and moisture resistant-Applied tape