3M 305
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Instant Acrylic Carton Closure
- Split-Resistant BOPP Handling
- Cold-Temperature Packaging Use
Product Description
Tartan Box Sealing Tape 305 is a 1.8 mil (0.046 mm) biaxially oriented polypropylene tape with a pressure-sensitive acrylic adhesive for general-purpose carton closure. The conformable backing wraps edges and rough recycled corrugate while resisting abrasion, moisture, scuffing, edge tear, and splitting during application. Instant adhesion requires no moisture, heat, or solvent activation, supporting smooth hand dispensing, manual dispensers, and case-sealing equipment. The clear or tan tape is intended for lightweight boxes exposed to minimal distribution hazards and performs in cold-temperature packaging work. It also resists yellowing, weathering, and UV exposure in lightweight carton-sealing service.
Key features
- Conformable BOPP backing: The polypropylene film follows carton edges and rough recycled corrugate for a tight closure.
- Instant acrylic adhesion: The pressure-sensitive adhesive requires no moisture, heat, or solvent activation.
- Split-resistant handling: The backing provides edge-tear and split resistance during carton-sealing application.
Applications
Suitable for lightweight carton sealing, food and beverage packaging, recycled liner paper and fiberboard, cold-temperature use, bag closure, and cartons exposed to UV light and aging.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Physical values are representative or typical and are not specification limits.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Clear and tan | - | Typical |
| Adhesive | Pressure-sensitive acrylic | - | As supplied |
| Backing | Biaxially oriented polypropylene film | - | As supplied |
| Backing thickness | 0.025 (1) | mm (mil) | Typical; ASTM D3652 |
| Total tape thickness | 0.046 (1.8) | mm (mil) | Typical; ASTM D3652 |
| Shelf life | 18 | months | From manufacture; 4 to 27 deg C and 40 to 50% RH |
Final-state / after-processing properties
Performance values are typical; methods and conditions are shown in each row.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180 deg peel adhesion | 17.7 (16.2) | N/100 mm (oz/in) | Typical; ASTM D3330; stainless steel, 23 deg C, 72 h dwell, 304 mm/min |
| Tensile strength | 701 (40) | N/100 mm (lb/in) | Typical; ASTM D3759; machine direction |
| Activation requirement | None | - | No moisture, heat, or solvent required |