3M 3302
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Low-Resistance Conductive Bonding
- Conformable EMI/RFI Shielding
- UL 510 Recognized Construction
Product Description
3M Conductive Aluminum Foil Tape 3302 is a silver, dead-soft aluminum foil tape with a conductive pressure-sensitive acrylic adhesive for low-level EMI/RFI shielding and printed-circuit manufacturing or repair. The 2 mil (0.05 mm) high-strength foil is malleable enough to follow irregular and textured surfaces, while the adhesive wets out to low-surface-energy materials and supports a low-resistance conductive bond. The 3.5 mil (0.09 mm) total construction is hand tearable for installation and carries UL 510 recognition. Applied performance includes typical peel and tensile data with long-term temperature resistance from -40 to 250 deg F (-40 to 121 deg C).
Key features
- Conductive acrylic interface: The adhesive supports low-resistance bonding and electrical continuity across the applied tape.
- Malleable dead-soft foil: The aluminum backing follows irregular, uneven, and difficult textured surfaces.
- Wide long-term temperature range: Applied tape is rated from -40 to 250 deg F (-40 to 121 deg C) for days or weeks.
Applications
Suitable for low-level EMI/RFI shielding, printed-circuit manufacturing and repair, grounding, and electrical-continuity applications.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
Physical values are representative or typical and are not specification limits.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Silver | - | Typical |
| Adhesive | Conductive acrylic | - | Pressure-sensitive |
| Backing | Dead-soft aluminum foil | - | As supplied |
| Backing thickness | 0.05 (2) | mm (mil) | Typical; ASTM D3652 |
| Total tape thickness | 0.09 (3.5) | mm (mil) | Typical; ASTM D3652 |
| Liner thickness | 0.11 (4.4) | mm (mil) | Typical |
| Shelf life | 12 | months | From manufacture; 16 to 27 deg C and 40 to 60% RH |
Final-state / after-processing properties
Performance values are typical; methods and conditions are shown in each row.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180 deg peel adhesion | 2.4 (21) | N/cm (oz/in) | Typical; ASTM D3330 at 23 deg C and 304 mm/min |
| Elongation at break | 3 | % | Typical; ASTM D3759 |
| Tensile strength | 33.3 (19) | N/cm (lb/in) | Typical; ASTM D3759 |
| Long-term temperature range | -40 to 121 (-40 to 250) | deg C (deg F) | Days or weeks |
| Recognition | UL 510 | - | File E230409 |