3M 4016
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- High-Shear Permanent Mounting
- Vibration-Damping Conformable Foam
- Protected 104 deg C Holding
Product Description
3M Double Coated Urethane Foam Tape 4016 is an off-white, open-cell urethane foam tape with acrylic pressure-sensitive adhesive on both sides for interior mounting and attachment. The 0.0625 in. (1.6 mm) flexible carrier conforms to joined surfaces, dampens vibration, and builds a strong permanent bond. 3M Adhesive 100 provides high ultimate adhesion, high shear holding power, and resistance to elevated temperatures, solvents, chemicals, and environmental exposure. The densified kraft-paper liner supports die-cutting and automated dispensing while limiting edge roll. This tape suits protected interior and exterior mounting, including signs, nameplates, dispensers, acoustic panels, wire clips, and corner protectors.
Key features
- High-Shear Acrylic Bond: 3M Adhesive 100 develops high ultimate adhesion and very high shear holding power.
- Conformable Vibration-Damping Foam: The flexible open-cell carrier follows surfaces and dampens vibration in mounted assemblies.
- Process-Stable Kraft Liner: The densified liner supports die-cutting and automated dispensing while reducing edge roll.
Applications
Suitable for protected mounting of interior signs, nameplates, dispensers, acoustic panels, wire clips, and corner protectors.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Carrier | Open-cell urethane foam | - | As supplied |
| Adhesive | Acrylic | - | Pressure-sensitive; both sides |
| Color | Off-white | - | As supplied |
| Total thickness without liner | 59 | mil | As supplied |
| Nominal product thickness | 0.0625 (1.6) | in (mm) | As supplied |
| Density | 11 | lb/ft3 | As supplied |
| Liner | 62 lb densified kraft paper | - | Green or green plaid |
| Shelf life | 24 | months | Product classification |
Final-state / after-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Elongation at break | 100 | % | Method not stated |
| Tensile strength | 140 | lb/in | Method not stated |
| Long-term holding temperature | Up to 220 (104) | deg F (deg C) | Applied tape |
| Bond development | Increases with natural aging | - | Applied tape |
| Resistance | Good temperature and chemical resistance | - | Applied tape |