3M 4200FC
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Fast Moisture-Cure Sealing
- Non-Sag Marine Application
- Flexible Bonds for Disassembly
Product Description
3M Marine Adhesive Sealant Fast Cure 4200FC is a one-part, moisture-curing polyurethane paste for bonding and sealing marine joints and hardware. Its medium-strength elastomeric seal is watertight and weather resistant while allowing later disassembly. At 73 deg F and 50% relative humidity, the typical tack-free time is 1 to 2 hours and the typical cure rate is 4 mm per 24 hours. The sealant can be used with wood, fiberglass, gelcoat, selected plastics, and metals; some plastics require testing and metals may require primer. It is used above and below the waterline on deck-to-hull joints, portholes, deck fittings, rub rails, screw holes, and stanchion supports.
Key features
- Fast Moisture Cure: Forms a tack-free surface in a typical 1 to 2 hours at 73 deg F and 50% relative humidity.
- Flexible Disassemblable Seal: The medium-strength elastomeric bond remains flexible and permits later disassembly.
- Non-Sag Marine Application: The caulkable paste stays non-sagging for marine joints and hardware above or below the waterline.
Applications
Suitable for fiberglass deck-to-hull joints, wood-to-fiberglass bonding, portholes, deck fittings, rub-rail attachment, screw holes, and stanchion supports.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
Technical values are representative or typical and are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Consistency | Caulkable, non-sag paste | - | Typical; as supplied |
| Density | 9.75 | lb/gal | Approximate; typical |
| Solids content | 100 | % | Approximate; typical |
| Tack-free time | 1 to 2 | hours | Typical at 73 deg F (23 deg C) and 50% RH |
| Rate of cure | 3/16 (4) | in (mm) per 24 h | Typical at 73 deg F (23 deg C) and 50% RH |
| Application surface temperature | 40 to 100 (4 to 38) | deg F (deg C) | Do not apply to frost-covered surfaces |
Final-state / after-processing properties
Technical values are representative or typical and are not specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shore A hardness | 40 | - | Typical; ASTM C661 |
| Tensile strength | 180 (1.24) | psi (MPa) | Typical; ASTM D412 |
| Elongation at break | >400 | % | Typical; ASTM D412 |
| Service temperature | -40 to 190 (-40 to 88) | deg F (deg C) | Typical product data |