3M 427
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Dead-Soft Aluminum Foil Backing
- Moisture-Barrier Tape Applications
- -54 to 149 deg C Temperature Resistance
Product Description
3M™ Aluminum Foil Tape 427 combines a nominal 3 mil dead-soft aluminum foil backing with a transparent acrylic adhesive and an easy-release paper liner. The tape provides a conformable metallic surface for industrial masking, holding, patching, sealing, splicing, and heat-reflective applications. Its low water-vapor transmission rate supports moisture-barrier uses, while the aluminum backing reflects heat and light. The tape is flame resistant, meets the requirements of FAR 25.853(a), and carries documented UL 746C and UL 723 Class “L” ratings.
Key features
- Conformable foil construction: Dead-soft aluminum backing conforms to surfaces for masking, holding, patching, sealing, and foil-splicing applications.
- Moisture and temperature performance: Provides a typical water-vapor transmission rate of 0.77 g/m²/24 h and long-term temperature resistance from -54°C to 149°C.
- Documented flame-performance requirements: Meets FAR 25.853(a), UL 746C, and UL 723 Class “L” requirements and can be certified to meet L-T-80C.
Applications / Suitable for
- Aircraft paint-stripping masking
- Moisture barriers in white-goods appliances
- General-purpose heat reflection and heat dissipation
- Holding wires and cooling coils in white-goods appliances
- Repairing tears on truck trailers and aircraft
- Splicing thin-gauge foils
- Indoor and outdoor holding, patching, and sealing
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical construction and physical properties of 3M™ Aluminum Foil Tape 427 as supplied. Values are representative and are not intended for specification purposes.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Shiny silver | — | Typical |
| Backing | Dead-soft aluminum | — | Typical construction |
| Adhesive type | Acrylic | — | Transparent adhesive |
| Backing thickness | 0.07 (2.8) | mm (mil) | ASTM D3652 |
| Total tape thickness | 0.12 (4.6) | mm (mil) | ASTM D3652; liner excluded |
| Liner | Easy-release paper | — | 0.08 mm (3.1 mil) liner thickness |
| Approximate weight | 5.54 (0.012) | g/m/24 mm (lb/yd/in) | Typical |
After-processing / final-state properties
Typical performance characteristics of 3M™ Aluminum Foil Tape 427. Values are representative and are not intended for specification purposes.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180° peel adhesion | 5.5 (50) | N/cm (oz/in) | ASTM D3330; 23°C (73°F); 304 mm/min (12 in/min) |
| Tensile strength | 49 (28) | N/cm (lb/in) | ASTM D3759 |
| Elongation at break | 6 | % | ASTM D3759 |
| Water-vapor transmission | 0.77 (0.05) | g/m²/24 h (g/100 in²/24 h) | ASTM D3833 |
| Long-term temperature resistance | -54 to 149 (-65 to 300) | °C (°F) | Long-term exposure defined as days or weeks |