3M 4298UV
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Fast 30-to-90-Second Drying
- Fluorescent Coverage Verification
- Multiple Application Methods
Product Description
3M Adhesion Promoter 4298UV is a fast-drying liquid primer that improves the adhesion of 3M Acrylic Foam Tape and 3M Acrylic Plus Tape to low- and medium-surface-energy plastics used in automotive trim and parts. At a recommended wet coating thickness of approximately 0.002 inch (0.05 mm) or less, the promoter typically dries in 30 to 90 seconds. A fluorescent dye makes the applied coating visible for coverage verification. It can be applied by gravity-feed wipe, knurled roller, sprayer, felt-tipped applicator, or a similar method. Applications include tape-bond surface preparation for TPO, TPU, polypropylene, EPDM, polycarbonate, acrylic, ABS, nylon, glass, TPV, and TPE.
Key features
- Rapid Drying: Dries in a typical 30 to 90 seconds at approximately 0.002 inch wet coating thickness, with time dependent on temperature and humidity.
- Visible Coverage Check: Fluorescent dye makes the applied promoter visible for coverage verification.
- Flexible Application Methods: Can be applied by gravity-feed wipe, knurled roller, sprayer, felt-tipped applicator, or a similar method.
Applications
Suitable for preparing specified automotive plastics and trim materials before applying compatible 3M Acrylic Foam Tape or 3M Acrylic Plus Tape.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Yellow | - | As supplied |
| Viscosity | <=25 | cP | Maximum |
| Drying time | 30 to 90 | seconds | Typical at approx. 0.002 in (0.05 mm) wet coating; varies with temperature and humidity |
| Coverage | 75 (800) | m^2/gal (ft^2/gal) | Based on 0.002 in wet coating thickness |
| Net weight | 820 (6.8) | g/L (lb/gal) | As supplied |
| Recommended wet coating thickness | <=0.002 (0.05) | in (mm) | Apply a thin, uniform coating |
| Tape application window | <=1 | hour | After promoter application; keep the primed surface free of contaminants |