3M™ VHB™ Tape 4910F
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- Clear Double Sided Tape
- Acrylic Adhesive
- Permanent Bonding for High Surface Energy Substrates
Product Description
3M™ VHB™ Tape 4910F is a clear, high-strength, double-sided acrylic foam tape designed for permanent bonding applications where a clean appearance and reliable adhesion to high surface energy (HSE) substrates are required. It combines a general-purpose acrylic adhesive with a clear acrylic foam core to provide durable bonding performance for applications involving metals, glass, and easy-to-bond painted surfaces and plastics.
3M™ VHB™ Tape 4910F features a 1.0 mm (40 mil) thick clear acrylic foam core with general-purpose acrylic adhesive on both sides. The firm acrylic foam construction provides a strong, durable bond while maintaining a virtually invisible fastening solution for transparent or translucent materials. The pressure-sensitive adhesive bonds on contact, providing immediate handling strength without the need for curing time.
The tape provides reliable bonding and sealing performance, creating a permanent seal against water and moisture. Its transparent construction allows it to be used in applications where maintaining the appearance of the bonded assembly is important. It can also replace mechanical fasteners such as rivets, screws, and welds, helping simplify assembly processes and eliminate drilling, grinding, and finishing operations.
Product Key Features
- Clear Acrylic Foam Construction – 1.0 mm (40 mil) transparent acrylic foam core provides a clean, nearly invisible bonding solution for applications where appearance is important.
- General-Purpose Acrylic Adhesive – Designed to provide strong adhesion to a wide range of high surface energy substrates including metals, glass, and painted surfaces.
- High-Strength Permanent Bonding – Delivers durable, long-term bonding performance for industrial assembly applications.
- Virtually Invisible Fastening – Clear tape construction helps maintain the aesthetics of bonded assemblies by eliminating visible fasteners.
- Bonding and Sealing Capability – Creates a permanent seal that helps protect against moisture and environmental exposure.
- Immediate Handling Strength – Pressure-sensitive adhesive bonds on contact, allowing efficient assembly without curing time.
- Replacement for Mechanical Fasteners – Can replace screws, rivets, welds, and other traditional fastening methods to simplify assembly processes.
- Thin, Lightweight Assembly Solution – Enables clean bonding of materials while reducing the need for additional hardware or fabrication steps.
Applications
3M™ VHB™ Tape 4910F is suited for permanent bonding applications requiring a transparent tape solution, strong adhesion, and long-term durability..
- Bonding transparent or translucent materials
- Joining glass and metal components
- Mounting decorative materials and trims
- Attaching nameplates and logos
- Panel-to-frame bonding applications
- Bonding stiffeners to panels
- Applications requiring replacement of mechanical fasteners or liquid adhesives
Technical Specifications
No specifications available.
Additional Information
3M® VHB®Tape 4910F
3M™ VHB™ Tape 4910F is a clear, double-coated acrylic foam tape designed for permanent bonding applications where a clean appearance and reliable adhesion are required. The acrylic adhesive on both sides provides strong bonding performance to a variety of high surface energy substrates, including metals, glass, and painted surfaces. The transparent acrylic foam core provides a virtually invisible bonding solution while maintaining durable attachment between substrates.
Note: Property values shown are typical and not intended for specification. Verify suitability under your geometry, dispense method, and cure profile.

Key Features
- Fast and easy to use
- Invisible fastening to keep surfaces smooth
- Allows the use of thinner, lighter-weight, and dissimilar materials
- Eliminates drilling, grinding, refinishing, screwing, welding and associated re-work
- Pressure-sensitive adhesive bonds on contact to provide immediate handling strength
Processing Summary
Typical Physical Properties
| Property | Typical value | Test method |
|---|---|---|
| Color | Clear | |
| Adhesive Type | General Purpose Acrylic | |
| Density | 960 kg/m³ | ASTM D3574 |
| Adhesive Carrier | Solid Acrylic | |
| Total Tape Thickness | 1 mm | ASTM D3652 |
| Thickness Tolerance | ±10 % | |
| Liner | Red PE Film 0.13 mm | |
| 90 Peel Adhesion | 26 N/cm | ASTM D330 |
| Normal Tensile | 690 kPa | ASTM D897 |
| Overlap Shear Strength | 480 kPa | ASTM D1002, ISO 4587 |
| Static Shear | 1000 g @ 23°C , 500 g @ 66°C , 500 g @ 93°C | |
| Minimum Application Temperature | 10 °C | |
| Short Term Temp Resistance | 149 °C | |
| Long Term Temp Resistance | 93 °C |
The manufacturing date is available on all 3M™ VHB™ Tapes as the lot number, typically marked on the core or on a label on the outer roll lap. The lot number, typically a 4 digit code, is a Julian date (Y D D D). The first digit refers to the year of manufacture, the last 3 digits refer to the days after January 1.
Example: A lot number of 7266 (or 17266) would translate to a date of manufacture of Sept. 23 (266th day of year) in 2017.
Surface Preparation and Application Techniques
Proper surface preparation and application technique are critical to achieving the maximum bond strength, durability, and long-term performance of 3M VHB™ Tape 5962F across a wide range of industrial substrates and operating conditions.
Exceptions that may require additional surface preparation include:
• Heavy Oils: A degreaser or solvent-based cleaner may be required to remove heavy oil or grease from a surface and
should be followed by cleaning with IPA/water.
• Abrasion: Abrading a surface, followed by cleaning with IPA/water, can remove heavy dirt or oxidation and can
increase surface area to improve adhesion.
• Adhesion Promoters: Priming a surface can significantly improve initial and ultimate adhesion to many materials such
as plastics and paints.
• Porous surfaces: Most porous and fibered materials such as wood, particleboard, concrete, etc. need to be sealed to
provide a unified surface.
• Unique Materials: Special surface preparation may be needed for glass and glass-like materials, copper and copper
containing metals, and plastics or rubber that contain components that migrate (e.g. plasticizers).
*Note: Initial tape application to surfaces at temperatures below these suggested minimums is not suggested because the adhesive becomes too firm to adhere readily. Ideally, all substrates and tape should be conditioned above the minimum application temperature in covered, weatherproof conditions until it is verified the substrates are at or above the minimum temperature. Once properly applied, low-temperature holding is generally satisfactory.
Bond Build Rate

After application, the bond strength will gradually increase as the adhesive flows onto to the surface (also referred to as “wet out”). The bond build rate will depend on both tape and substrate, but generally, at room temperature, approximately 50% of ultimate bond strength will be achieved after 20 minutes, 90% after 24 hours, and 100% after 72 hours. Adhesive flow is faster at higher temperatures and slower at lower temperatures. Ultimate bond strength can be accelerated (and in some cases bond strength can be increased) by exposure to elevated temperature (e.g. 66°C [150°F] for 1 hour). This can provide better adhesive wet out onto the substrates. Abrasion (~180 grit), or the use of primers/adhesion promoters, can also increase both bond strength as well as the bond build rate.
Tips and Troubleshooting
| Issue | Recommended Action |
|---|---|
| Adhesion |
Adhesion to the substrate is critical to achieving high bond strength. Adhesives must flow onto the substrate surfaces in order to achieve an intimate contact area and allow the molecular force of attraction to develop. The degree of flow of theadhesive on the substrate is largely determined by the surface energy of the substrate. |
| Tape Usage |
Use the right amount of VHB™ Tape to handle the expected stresses. Because 3M™ VHB™ Tapes are viscoelastic by |
| Tape Thickness |
Achieving good contact is also important. The necessary thickness of tape depends on the rigidity of substrates as well |
| Thermal Expansion/Contraction |
3M™ VHB™ Tapes perform well in applications where two bonded surfaces may expand and contract at different rates. |
| Bond Flexibility |
While an advantage for many applications where allowing differential movement is a benefit, the tape bonds are |