3M 4950
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Immediate No-Cure Assembly Handling
- Firm 1.1 mm Foam Bonding
- High-Surface-Energy Permanent Attachment
Product Description
3M VHB Tape 4950 is a white, double-sided acrylic foam tape for permanent bonding of metals, glass, and other high-surface-energy materials. A firm acrylic foam core with general-purpose acrylic adhesive provides a 1.1 mm tape thickness and immediate handling strength without a fixturing or cure wait. The tape is rated for long-term use up to 93 deg C and short-term exposure up to 149 deg C for up to four hours. Its permanent bonding format is used for stiffener-to-panel and panel-to-frame attachment, decorative trim, nameplates, and logos.
Key features
- Immediate no-cure handling: Pressure-sensitive all-acrylic bonding develops immediate handling strength without a fixturing or cure wait.
- Firm 1.1 mm foam core: The firm acrylic foam construction provides a 1.1 mm double-sided bonding layer for permanent attachment.
- High-surface-energy bonding: General-purpose acrylic adhesive bonds metals, glass, and other documented high-surface-energy substrates.
Applications
Applications include stiffener-to-panel bonding, panel-to-frame attachment, decorative trim, nameplates, and logos.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | White | Tape body | |
| Adhesive type | General-purpose acrylic | Both sides | |
| Core | Firm acrylic foam | Double-sided construction | |
| Total tape thickness | 1.1 | mm | 45 mil; product thickness |
| Liner material | Densified kraft paper | Release liner |