3M 550FC
Harmonization Code : 3919.10.80 | Other self-adhesive plastic rolls not exceeding 20 cm wide.
Main features
- One-Component Fast Moisture Cure
- High Tensile Strength and Modulus
- Water and Salt-Spray Resistance
Product Description
3M™ Polyurethane Adhesive Sealant Fast Cure 550 is a fast-curing, one-component, moisture-curing polyurethane sealant that forms permanently elastic bonds. It is designed to bond a wide variety of dissimilar materials including plastics, metals, fiberglass, and wood, offering high tensile strength suitable for fastener replacement. This versatile adhesive sealant features a high modulus and Shore A hardness for robust bonding, and it is paintable after curing to improve the final product finish.
Key features
- Fast-curing, one-component formula: Moisture-curing system requires no mixing, simplifying production and assembly processes.
- Permanently elastic and strong: Features high tensile strength for potential fastener replacement and a high modulus for stronger, durable bonds.
- Excellent substrate versatility: Readily bonds dissimilar materials like plastics, metals, fiberglass, and wood to provide design flexibility.
Applications / Suitable for
- General industrial, construction, marine, and specialty vehicle bonding
- Marine deck to hull bonding
- Sealing and bonding diverse, dissimilar materials
Technical Specifications
General Properties
Mechanical Properties
Thermal Properties
Other Properties
Physical Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Consistency | Medium Paste | - | - |
| Specific Gravity | 1.17 | - | - |
| VOC | 29 | g/L | (0.242 lb/gal) |
| Approximate Coverage | 38 | lineal m | 10.5 oz. cartridge, 1/8 in (3 mm) bead (126 LF) |
| Application Temperature | 5-35 | °C | (40-95°F) |
| Tack Free Time | 50-90 | minutes | at 23°C (73°F) |
| Rate of Cure | 4 | mm/24 h | at 23°C (73°F) (3-16 in/24 h) |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shore A Hardness | 45 | - | ASTM C661 |
| Modulus at 100% Elongation | 1 | MPa | ASTM D412 at 23°C (73°F) (150 lb/in²) |
| Tensile Strength | 3.1 | MPa | ASTM D412 (450 lb/in²) |
| Elongation at Break | > 600 | % | ASTM D412 |
| Long Term Temperature Resistance | 90 | °C | (194°F) |
| Minimum Long Term Temperature Resistance | -40 | °C | (-40°F) |