3M 7448
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Ultra Fine Silicon-Carbide Finishing
- Conformable Access to Irregular Surfaces
- Load-Resistant Long-Life Open Web
Product Description
Scotch-Brite Hand Pad 7448 is an Ultra Fine silicon carbide nonwoven abrasive pad for cleaning, blending, surface preparation, and final finishing. The conformable pad reaches irregular surfaces and corners, while its load- and heat-resistant open web maintains consistent abrasive action during use. The silicon carbide mineral provides a fine finishing action, and the pad performs similarly to steel wool grade 00 without shredding, rusting, or leaving metal splinters. It can be used by hand, with a hand-pad block, or on an in-line sander for surface-conditioning work.
Key features
- Ultra Fine silicon carbide: The sharp silicon carbide mineral delivers fine finishing action for cleaning, blending, preparation, and finishing.
- Conformable corner access: The pad reaches irregular surfaces and corners without losing finishing performance.
- Load-resistant open web: The heat- and load-resistant nonwoven web runs clean and maintains consistent abrasive action.
Applications
Use it for cleaning, blending, final finishing, and pre-paint surface preparation on metals, wood, plastics, and composites.
Technical Specifications
No specifications available.
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Grade | Ultra Fine | As supplied | |
| Abrasive material | Silicon carbide | As supplied | |
| Construction | Nonwoven open-web hand pad | As supplied | |
| Color | Gray | As supplied |