3M 76
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- High-Tack Industrial Formulation Excels in One-Surface Bonding
- Polyethylene and Polypropylene Bonding
- Controlled Variable Lace Spray Pattern
Product Description
3M™ Hi-Tack 76 Spray Adhesive is an industrial aerosol spray adhesive formulated with high tack for single-surface bonding applications. This translucent, synthetic elastomer-based adhesive effectively bonds hard-to-hold materials such as polyethylene and polypropylene. It provides a variable lace spray pattern and is an excellent choice for adhering fabric headliners, rubber, felt, plastics, and foil to themselves or to wood and metal surfaces.
Key features
- High-tack performance: Formulated specifically for efficient one-surface bonding applications with a rapid 1-2 minute dry time.
- Bonds difficult substrates: Effectively adheres to hard-to-hold plastics, including polyethylene and polypropylene.
- Variable lace spray: Aerosol delivery provides a controlled variable lace pattern for precise application and a coverage of up to 2.6 m² (28 ft²) per can.
Applications / Suitable for
- One-surface bonding applications
- Bonding polyethylene and polypropylene plastics
- Attaching fabric headliners
- Bonding rubber, felt, cardboard, cork, and foil to wood or metal
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Base | Synthetic Elastomer | - | - |
| Color | Translucent | - | - |
| Spray Pattern | Variable Lace | - | - |
| Solids Content by Weight | 13.5 | % | - |
| Density | 0.78 | kg/L | (6.5 lb/gal) |
| Coverage | 2.6 | m² | (28 ft²) at 27 g/m² dry |
| Dry Time | 1-2 | minutes | Dependent on ambient conditions and coverage |
| Bonding Range | 1-10 | minutes | 1 surface |
| Bonding Range | 1-60 | minutes | 2 surfaces |
After-processing / final-state properties
Typical properties; these values are not intended for use in preparing specifications.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Shear Adhesion Failure Test (SAFT) | 110 | °C | 230°F (birch plywood, 25 mm overlap, 100 g) |