3M 8417
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Transparent Self-Wound Polyester Film
- Edge-Tear-Resistant Film Backing
- -40 to 93 deg C Exposure Range
Product Description
3M™ PET Durable Label Material 8417 is a transparent, self-wound polyester film coated with 3M™ Adhesive 100 High-temperature Acrylic. Commonly used as an overlaminate with 3M™ PET Durable Label Material 8418, it provides instant adhesion, transparency, and a tough film backing that resists edge tearing during processing and dispensing. The construction also offers documented chemical resistance and stability across elevated and low-temperature exposure conditions, supporting durable identification applications where environmental resistance is required. :contentReference[oaicite:0]{index=0}
Key features
- Transparent overlaminate construction: Clear polyester film preserves label visibility when used as an overlaminate.
- Durable film backing: Tough polyester resists edge tearing during processing and dispensing.
- Environmental resistance: Documented exposure testing shows no appearance change after selected chemical, humidity, and temperature conditions.
Applications / Suitable for
- Overlaminating 3M™ PET Durable Label Material 8418
- Fluid-line identification
- General identification applications requiring chemical and temperature resistance
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Typical construction, dimensional, dispensing, and storage properties of 3M™ PET Durable Label Material 8417. Values are representative and are not intended for specification purposes. :contentReference[oaicite:1]{index=1}
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Construction | Self-wound transparent polyester film | — | Linerless construction |
| Adhesive type | 3M™ Adhesive 100 High-temperature Acrylic | — | Typical construction |
| Total tape thickness | 0.056 (2.2) | mm (mil) | ASTM D3652; nominal caliper |
| Adhesive thickness | 0.03 (1.2) | mm (mil) | Nominal caliper |
| Facestock thickness | 0.025 (1) | mm (mil) | Polyester facestock; nominal caliper |
| Typical unwind | 3 (3) | oz/in (N/100 mm) | Shocky unwind |
| Shelf life | 24 | months | From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging away from direct sunlight |
After-processing / final-state properties
Typical adhesion, mechanical, chemical, and temperature-exposure characteristics of 3M™ PET Durable Label Material 8417. Values are representative and are not intended for specification purposes. :contentReference[oaicite:2]{index=2}
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180° peel adhesion — ABS | 3.8 (35) | N/cm (oz/in) | ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min) |
| 180° peel adhesion — glass | 4.9 (45) | N/cm (oz/in) | ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min) |
| 180° peel adhesion — polypropylene | 1.2 (11) | N/cm (oz/in) | ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min) |
| 180° peel adhesion — stainless steel | 4.1 (38) | N/cm (oz/in) | ASTM D3330; 23°C (73°F); 10 min dwell; 304 mm/min (12 in/min) |
| Tensile strength | 43.5 (400) | N/cm (oz/in) | Typical |
| Elongation at break | 100 | % | Typical |
| Chemical exposure appearance | No change | — | 4 h immersion at room conditions; 2 × 2 in samples on stainless steel; tested with isopropyl alcohol, 10W30 oil, pH 4 acid, pH 10 base, and water; zero edge penetration |
| Temperature-exposure appearance | No change | — | 24 h exposure; 2 × 2 in samples on stainless steel; tested from -40°C (-40°F) to 93°C (200°F); selected conditions also evaluated at 90% RH |