3M 853
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- 0.06 mm Thin Tape Construction
- Solvent-Resistant Tape Adhesive
- Transparent Label-Protection Tape
Product Description
3M™ Polyester Tape 853 is a transparent polyester film tape with a high-shear, solvent-resistant acrylic adhesive. Its thin, high-strength construction provides reliable bonding without obscuring protected information, making it suitable for high-tension splicing, critical label protection, tape hinges, and moisture-sealing applications. The tape withstands long-term temperatures from -50 to 150°C (-60 to 300°F) and resists solvents including jet engine fuel, hydraulic fluid, and lubricating oils.
Key features
- Thin, strong construction: Combines a 0.03 mm (1.1 mil) polyester backing with a total tape thickness of 0.06 mm (2.2 mil).
- Solvent-resistant adhesion: Acrylic adhesive resists many solvents, including jet engine fuel, hydraulic fluid, and lubricating oils.
- Transparent protection: Allows information beneath the tape to remain visible during label-protection and sealing applications.
- Broad temperature resistance: Supports long-term use from -50 to 150°C (-60 to 300°F).
- Aerospace flammability performance: Meets FAR 25.853(a), Appendix F, Part I (a)(1)(ii), and can be qualified to Federal Specification L-T-100 Type I.
Applications / Suitable for
- High-tension splicing
- Critical label protection
- Tape hinges
- Aerospace applications requiring FAR flammability performance
- Sealing critical areas against moisture intrusion
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Representative or typical product properties. Values should not be used for specification purposes.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product construction | Polyester backing with acrylic adhesive | — | As supplied |
| Color | Transparent | — | As supplied |
| Backing thickness | 0.03 (1.1) | mm (mil) | ASTM D3652 |
| Total tape thickness | 0.06 (2.2) | mm (mil) | ASTM D3652 |
| 180° peel adhesion | 5 (46) | N/cm (oz/in) | ASTM D3330; 23°C (73°F); 304 mm/min (12 in/min) |
| Tensile strength | 43.4 (25) | N/cm (lb/in) | ASTM D3759 |
| Elongation at break | 83 | % | ASTM D3759 |
| Water vapor transmission | 15.5 (1) | g/m²/24 h (g/100 in²/24 h) | ASTM D3833 |
| Minimum long-term temperature resistance | -50 (-60) | °C (°F) | Long term: days or weeks |
| Maximum long-term temperature resistance | 150 (300) | °C (°F) | Long term: days or weeks |
| Standard roll length | 65.8 (72) | m (yd) | Published standard size |
| Shelf life | 18 | months | From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging and out of direct sunlight |