3M 8934
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Glass-Reinforced Packaging Strength
- Minimal-Rubdown Package Reinforcement
- Transparent Reinforcement Preserves Graphics
Product Description
Tartan Filament Tape 8934 is a clear glass-yarn reinforced BOPP tape with pressure-sensitive synthetic rubber-resin adhesive for light-duty strapping and package reinforcement. The 0.102 mm construction combines good initial adhesion with high tensile and shear strength, while the transparent backing keeps box graphics and printing visible. Typical performance includes 53 N/100 mm 180 deg peel adhesion to stainless steel after 72 hours at 23 deg C, 3% elongation at break, and 175.1 N/cm tensile strength. Application is easiest at room temperature.
Key features
- Glass-yarn tensile reinforcement: Glass yarn filaments add tensile strength for box closing, bundling, reinforcing, and pallet unitizing.
- Low-rubdown initial adhesion: Synthetic rubber-resin adhesive develops good initial adhesion and holds with minimal rub-down on common packaging surfaces.
- Transparent protective backing: Clear BOPP construction keeps graphics visible while resisting nicks, abrasion, moisture, and scuffing.
Applications
Applications include box closing and reinforcement, light-duty strapping, bundling, sealing, palletizing, and intra-plant movement of packaged goods.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Other Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesive type | Pressure-sensitive synthetic rubber-resin | As supplied | |
| Backing | Biaxially oriented polypropylene (BOPP) | Clear backing | |
| Fiber reinforcement | Glass yarn | As supplied | |
| Total tape thickness | 0.102 | mm | ASTM D3652; typical |
| Shelf life | 18 | months | Original packaging; 4 to 27 deg C and 40 to 50% RH |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| 180 deg peel adhesion | 53 | N/100 mm | ASTM D3330; stainless steel; 72 h dwell; 23 deg C; typical |
| Elongation at break | 3 | % | ASTM D3759; typical |
| Tensile strength | 175.1 | N/cm | ASTM D3759; typical |