3M 92
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Polyimide Film with Silicone Adhesive
- 6,000 V Dielectric Breakdown
- UL-Recognized Flame-Retardant Tape
Product Description
3M™ Polyimide Film Electrical Tape 92 with Silicone Adhesive is an amber electrical tape constructed with a polyimide film backing and a non-corrosive, thermosetting silicone pressure-sensitive adhesive. The 2.75 mil (0.070 mm) tape is designed for continuous operation at temperatures not exceeding 180°C (356°F) per its UL listing. It is commonly used for electrical insulation, component wrapping, lead anchoring, and solder masking during printed circuit board assembly.
Key features
- High-temperature electrical tape: Designed for continuous operation at temperatures not exceeding 180°C (356°F) per its UL listing.
- Polyimide film construction: Combines a nominal 1 mil (0.025 mm) polyimide backing with a thermosetting silicone pressure-sensitive adhesive.
- Electrical insulation performance: Provides a minimum dielectric breakdown of 6,000 V and minimum insulation resistance of 1 × 1012 Ω.
- Non-corrosive adhesive: Delivers an electrolytic corrosion factor of 1.0, where 1.0 indicates no corrosion observed under 3M Test Method ETM-54001.
- Pressure-sensitive application: Requires no heat, moisture, or other preparation to achieve application.
Applications / Suitable for
- Wrapping coils, capacitors, wire harnesses, and transformers
- Anchoring electrical leads
- Solder masking during printed circuit board assembly
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Published product properties measured at 73°F (23°C) unless otherwise stated.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Amber | — | Visual |
| Backing | Polyimide film | — | As supplied |
| Adhesive | Thermosetting silicone | — | Pressure-sensitive adhesive |
| Backing thickness, nominal | 1 (0.025) | mil (mm) | Published nominal value |
| Total thickness | 2.75 ± 0.75 (0.070 ± 0.019) | mil (mm) | ASTM D1000; 73°F (23°C) |
| Adhesion to steel, minimum | 18 (2.0) | oz/in (N/cm) | ASTM D1000; 73°F (23°C) |
| Breaking strength, minimum | 20 (35) | lb/in (N/cm) | ASTM D1000; 73°F (23°C) |
| Elongation, minimum | 40 | % | ASTM D1000; 73°F (23°C) |
| Dielectric breakdown, minimum | 6,000 | V | ASTM D1000; 73°F (23°C) |
| Insulation resistance, minimum | 1 × 1012 | Ω | ASTM D1000; 73°F (23°C) |
| Electrolytic corrosion factor | 1.0 | — | 3M ETM-54001; 1.0 indicates no corrosion observed |
| Flame retardancy | Pass | — | UL Recognized flame retardant per UL 510A |
| Continuous operating temperature, maximum | 180 (356) | °C (°F) | Per UL listing |
| Shelf life | 5 | years | From date of manufacture; store at 50–80°F (10–27°C) and less than 75% relative humidity |