3M 950

Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others

3M 950

Main features

  • 5 mil Adhesive 300 Construction
  • High Initial Adhesion and Holding
  • Multi-Substrate Pressure-Sensitive Bonding

Product Description

3M™ Adhesive Transfer Tape 950 is a 5 mil (0.13 mm) adhesive transfer tape featuring 3M™ Adhesive 300, a pressure-sensitive, medium-firm, fibered acrylic adhesive supplied on a tan 60# glassine liner. It provides very high initial adhesion with good holding power across a range of materials, including metals, foams, fabrics, coated papers, and high- and low-surface-energy plastics.

Key features

  • High initial adhesion: 3M™ Adhesive 300 provides strong initial bonding with good holding power.
  • Broad substrate compatibility: Bonds to metals, foams, fabrics, coated papers, and high- and low-surface-energy plastics.
  • Conformable 5 mil adhesive: The 0.13 mm adhesive thickness supports bonding to surfaces where texture may be visible.
  • Environmental resistance: Provides resistance to humidity, water, UV exposure, temperature cycling, oil, mild acids, and mild alkalis when properly applied.
  • UL-recognized construction: Recognized under UL 969 for Marking and Labeling Systems Materials Components.

Applications / Suitable for

  • Bonding graphic nameplates and overlays
  • Attaching metal nameplates and rating plates
  • Laminating foam for gasket applications
  • Joining similar and dissimilar industrial materials
Product Family

3M 950

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Adhesive Layer Adhesive Layer
300 Fibered Acrylic
Release Liner Release Liner
Tan 60# Glassine
Total Thickness Total Thickness
130 μm

Additional Information

Technical properties

As-supplied / before-processing properties

Representative or typical product properties. Values should not be used for specification purposes.

Property Value Unit Method / condition
Adhesive type 3M™ Adhesive 300, fibered acrylic — Pressure-sensitive, medium-firm acrylic
Total tape thickness 0.13 (5) mm (mil) ASTM D3652
Liner 60# glassine — Tan primary liner
Liner thickness 0.08 (3.2) mm (mil) Published typical value
90° peel adhesion — ABS 3.7 (34); 4.4 (40) N/cm (oz/in) ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min)
90° peel adhesion — polypropylene 6.6 (60); 6.8 (62) N/cm (oz/in) ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min)
90° peel adhesion — stainless steel 8.1 (74); 9.4 (86) N/cm (oz/in) ASTM D3330; 15 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min)
Short-term temperature resistance 121 (250) °C (°F) Short term: minutes or hours
Long-term temperature resistance 70 (158) °C (°F) Long term: days or weeks
Lower temperature service limit -40 (-40) °C (°F) Properly applied tape
Coefficient of thermal expansion — first heat 20 × 10-5 m/m/°C ASTM D696
Coefficient of thermal expansion — second heat 58 × 10-5 m/m/°C ASTM D696
Dielectric constant 3.21 — ASTM D150; 23°C (73°F); 1 kHz
Dissipation factor 0.04 — 23°C (73°F); 1 kHz
Dielectric strength 340 V/mil ASTM D149; 500 VAC RMS, 60 Hz/sec
Shelf life 24 months From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in original packaging and out of direct sunlight