3M 966
Harmonization Code : 3910.00.00.90 | Silicones in Primary Forms; Others
Main features
- Up to 232 deg C Short-Term Exposure
- 10,000-Minute Static Shear
- Metal and High-Energy-Plastic Bonding
Product Description
3M™ Adhesive Transfer Tape 966 is a 2.3 mil (0.06 mm) adhesive transfer tape featuring 3M™ High Temperature Acrylic Adhesive 100 on a 62# densified kraft liner. It provides excellent bonding to metals and high-surface-energy plastics, exceptional static shear performance at elevated temperatures, and resistance to demanding chemical and environmental exposure. Its low-outgassing and low-leachable-chloride characteristics make it suitable for evaluated electronic, aerospace, industrial labeling, nameplate, and die-cutting applications.
Key features
- High-temperature performance: Supports short-term exposure up to 232°C (450°F) and long-term exposure up to 204°C (400°F).
- Exceptional static shear: Achieves 10,000-minute static shear results at temperatures from 23 to 232°C under the published test conditions.
- Strong high-surface-energy bonding: Provides excellent adhesion to metals and good adhesion to high-surface-energy plastics.
- Environmental and chemical resistance: Resists humidity, water, UV exposure, temperature cycling, gasoline, oil, mild acids, and mild alkalis when properly applied.
- Low-outgassing construction: Offers low outgassing and low leachable chloride for evaluated electronic and aerospace applications.
Applications / Suitable for
- Bonding metal nameplates
- High-temperature labels and identification components
- Die-cut parts requiring a densified kraft liner
- Evaluated electronic, aerospace, and industrial applications
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Representative or typical product properties. Values should not be used for specification purposes.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Adhesive type | 3M™ High Temperature Acrylic Adhesive 100 | — | Pressure-sensitive acrylic adhesive |
| Total tape thickness | 0.06 (2.3) | mm (mil) | ASTM D3652 |
| Liner | 62# densified kraft with “3M” printed in green | — | As supplied |
| Liner thickness | 0.09 (3.6) | mm (mil) | Published typical value |
| 90° peel adhesion — ABS | 4.8 (44); 5.9 (54) | N/cm (oz/in) | ASTM D3330; 20 min and 72 h dwell; 23°C (73°F); 2 mil aluminum-foil backing; 304 mm/min (12 in/min) |
| 90° peel adhesion — stainless steel | 5.8 (53); 8.5 (78) | N/cm (oz/in) | ASTM D3330; 20 min and 72 h dwell; 23°C (73°F); 2 mil PET backing at 20 min and 2 mil aluminum-foil backing at 72 h; 304 mm/min (12 in/min) |
| Static shear — 23°C (73°F) | 10,000 | minutes | ASTM D3654; 2,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes |
| Static shear — 70°C (158°F) | 10,000 | minutes | ASTM D3654; 1,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes |
| Static shear — 93°C (200°F) | 10,000 | minutes | ASTM D3654; 1,000 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes |
| Static shear — 232°C (450°F) | 10,000 | minutes | ASTM D3654; 400 g load; 25 × 25 mm (1 × 1 in) sample; test terminated after 10,000 minutes |
| Short-term temperature resistance | 232 (450) | °C (°F) | Short term: minutes or hours |
| Long-term temperature resistance | 204 (400) | °C (°F) | Long term: days or weeks |
| Low-temperature service | -40 (-40) | °C (°F) | Parts should be tested for low-temperature shock service |
| Thermal conductivity | 0.178; 0.183; 0.187 | W/m/K | ASTM C518; at 41°C (107°F), 71°C (160°F), and 101°C (214°F), respectively |
| Dielectric constant | 2.92 | — | ASTM D150; 23°C (73°F); 1 kHz |
| Dissipation factor | 0.025 | — | ASTM D150; 23°C (73°F); 1 kHz |
| Dielectric strength | 1,100 | V/mil | ASTM D149; 500 VAC RMS; 60 Hz/sec |
| Volume resistivity | 4 × 1015 | Ω·cm | ASTM D257; 23°C (73°F) |
| Application temperature range | 21 to 38 (70 to 100) | °C (°F) | Ideal range; application below 10°C (50°F) is not recommended for most pressure-sensitive adhesives |
| Shelf life | 24 | months | From date of manufacture; store at 16–27°C (60–80°F), 40–60% RH, in a sealed plastic bag and out of direct sunlight |