3M AF126-2

Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg

3M AF126-2

Main features

  • Low Temperature Cure
  • Controlled Low Flow Processing
  • Clean Low Tack Layup

Product Description

3M Scotch-Weld Structural Adhesive Film AF 126-2 is a toughened epoxy structural adhesive film for bonding prepared metal, composite, and honeycomb assemblies. The matte nonwoven scrim-supported construction is available in several nominal weights and calipers, with low tack that supports clean handling during layup. Low flow during cure helps control the bondline, and the film can cure at temperatures as low as 82 deg C. Film weight, primer, metal preparation, pressure, and cure schedule define the complete bonding process.

Key features

  • Low Temperature Cure: The film can cure at temperatures as low as 82 deg C.
  • Low Flow Bondline Control: Controlled flow helps maintain adhesive placement during cure.
  • Low Tack Layup Handling: The supported film is designed for clean positioning before cure.

Applications

Structural bonding of prepared metals, composites, and honeycomb sandwich assemblies.

Product Family

3M AF126-2

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Blue
Physical Properties
Volatiles Volatiles
Less than 1 %
Other Properties
Storage Temperature Storage Temperature
-18 °C

Additional Information

Technical properties

As-supplied / before-processing properties

Values are listed by AF 126-2 film weight to preserve configuration context.

PropertyValueUnitMethod / condition
Film constructionMatte nonwoven scrim supported-AF 126-2
Nominal areal weight options147; 294; 392g/m20.030; 0.060; 0.080 lb/ft2 variants
Nominal caliper options0.13; 0.25; 0.38mmCorresponding weight variants
Color by weightBlue-gray; blue-gray; blue-Corresponding weight variants
Volatile contentLess than 1%As supplied
Technical properties

After-processing / final-state properties

Cured bond averages retain film-weight and EC-2320 primer context.

PropertyValueUnitMethod / condition
Tensile shear at 24 deg C, 0.030 wt32.8MPaAverage with EC-2320 primer
Tensile shear at 24 deg C, 0.060 wt35.8MPaAverage with EC-2320 primer
Tensile shear at 24 deg C, 0.080 wt38.5MPaAverage with EC-2320 primer
T-peel at 24 deg C, 0.030 wt125N/25 mmAverage with EC-2320 primer
T-peel at 24 deg C, 0.060 wt182N/25 mmAverage with EC-2320 primer