3M™ Scotch-Weld™ Epoxy Adhesive DP190
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- 90-minute work life
- 1:1 mix ratio
- High shear and peel strength
Product Description
3M™ Scotch-Weld™ Epoxy Adhesive DP190 is a versatile, two-part epoxy designed for strong, durable bonding with a convenient 1:1 mix ratio. Available in both translucent and grey variants, this adhesive offers reliable performance across a range of materials while maintaining flexibility and resistance to environmental stress. It is formulated to deliver excellent handling properties and consistent results, making it suitable for industrial and general-purpose applications.
Product Key Features
- Convenient 1:1 mix ratio for easy and accurate dispensing
- Extended 90-minute work life for improved positioning and assembly time
- High shear and peel strength for durable, long-lasting bonds
- Flexible formulation to accommodate movement and reduce stress on bonded joints
- Available in translucent or grey to suit different application and aesthetic needs
- Excellent environmental resistance, including aging performance
- Consistent performance comparable to 3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A, with faster curing (translucent variant)
- Suitable for bulk and cartridge applications for production efficiency