3M DP605NS
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Tough Flexible Urethane Bond
- Five Minute Assembly Work Life
- Non Sag Placement Control
Product Description
3M Scotch-Weld Urethane Adhesive DP605NS, Off-White is a two-part, non-sag urethane adhesive that forms tough, flexible bonds on prepared wood, selected plastics, painted metals, ceramics, and glass. The 1:1 mix ratio and 5 minute work life support fast assembly, while the thixotropic consistency controls placement on vertical or contoured joints. Handling strength develops in 15 to 20 minutes at 23 deg C. The cured off-white adhesive combines 100% elongation with peel and overlap-shear performance for assemblies that require flexibility.
Key features
- Tough Flexible Urethane Bond: The cured adhesive combines structural attachment with 100% elongation.
- Five Minute Assembly Work Life: The fast work life supports rapid placement and fixturing.
- Non Sag Placement Control: Thixotropic consistency resists running on vertical and contoured joints.
Applications
Bonding prepared wood, selected plastics, painted metals, ceramics, glass, and flexible industrial assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Other Properties
Electrical Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Part B color | White | - | Before mixing |
| Part A color | Tan | - | Before mixing |
| Mix ratio by volume | 1:1 | B:A | Two-part system |
| Mix ratio by weight | 1:1 | B:A | Two-part system |
| Part B density | 8.8 to 9.2 | lb/gal | As supplied |
| Part A density | 9.7 to 10.2 | lb/gal | As supplied |
| Work life | 5 | min | 10 g mass, 1/4 in thick at 23 deg C |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Off white | - | Cured |
| Hardness | 60 to 65 | Shore D | ASTM D2240 |
| Elongation | 100 | % | ASTM D882 basis |
| Glass transition temperature | 41 | deg C | DSC, second heat |
| Overlap shear on aluminum | 650 | psi | ASTM D1002 at 23 deg C; MEK, abrade, MEK preparation |
| Floating roller peel on aluminum | 33 | piw | ASTM D3167 at 23 deg C |