3M DP8625NS

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

3M DP8625NS

Main features

  • Flexible Dissimilar Material Bonding
  • Controlled Non Sag Dispensing
  • Extended Panel Assembly Window

Product Description

3M Scotch-Weld Flexible Acrylic Adhesive DP8625NS is a black, low-odor, non-flammable acrylic structural adhesive supplied in a 10:1 cartridge system for static-mixer dispensing. The non-sag paste holds its shape in vertical joints, panel seams, and gaps between steel, aluminum, composites, and selected plastics. A 21 minute open time provides a defined positioning window, and handling strength develops in approximately 28 minutes at 23 deg C. After seven days, the cured adhesive reaches 200% elongation and Shore D 35 hardness for flexible dissimilar-material assemblies.

Key features

  • Flexible Dissimilar Material Bonding: The cured acrylic supports compatible metal, composite, and plastic assemblies.
  • Non Sag Cartridge Dispensing: The 10:1 paste formulation controls placement through a static mixer.
  • Extended Assembly Window: A 21 minute open time supports positioning before parts are fixed.

Applications

Panel-to-frame bonding, thin-panel assembly, dissimilar-material joining, and controlled gap filling with compatible substrates.

Product Family

3M DP8625NS

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Component System Component System
Two (Base / Accelerator)
Other Properties
Storage Temperature Storage Temperature
16 - 27 °C
Mechanical Properties
Elongation Elongation
118 %
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
27 °C
Thermal Conductivity Thermal Conductivity
0.233 W/m.K

Additional Information

Technical properties

As-supplied / before-processing properties

PropertyValueUnitMethod / condition
Mix ratio by volume10:1Base:acceleratorTwo-part cartridge system
Base colorBlack-Before mixing
Accelerator colorGray-Before mixing
Base density1.11g/cm3At 23 deg C
Accelerator density1.08g/cm3At 23 deg C
ViscosityNon-sag paste-As supplied
Open time21minMixed adhesive at 23 deg C
Time to handling strength28minMixed adhesive at 23 deg C
Technical properties

After-processing / final-state properties

PropertyValueUnitMethod / condition
ColorBlack-Cured
Tensile modulus0.7MPaASTM D638 after 7 days at 23 deg C
Tensile stress at break1.48MPaASTM D638 after 7 days at 23 deg C
Elongation at break200%ASTM D638 after 7 days at 23 deg C
Hardness35Shore DASTM D2240 after 7 days at 23 deg C
Glass transition temperature28deg CDynamic mechanical analysis after 7 days

Leading Brands Trust in Our Products and Services

Products that Perform| Knowledge that Serves| Service that Delivers