3M Scotch-Weld Urethane Adhesive EC-3549 B/A is a two-part, sag-resistant urethane adhesive for tough structural bonds on many primed or painted metals, plastics, wood, and composites. The mixed material resists sagging in approximately 30 seconds, helping control bead placement on vertical and irregular joints. A 60 minute work life provides time for application, alignment, and adjustment before cure at room temperature or with heat. On etched aluminum, published overlap shear reaches 2000 psi at 24 deg C and 2500 psi at -40 deg C under the specified test configuration.
Key features
- High Peel Structural Bonding: The tough polyurethane is formulated for durable bonds with high peel strength.
- Impact Resistant Performance: The cured adhesive tolerates shocks and collisions in structural assemblies.
- Sag Resistant Placement: The mixed material resists sagging in approximately 30 seconds for accurate application.
Applications
Bonding compatible primed or painted metals, plastics, wood, and composites in tough structural assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Product type | Two-part urethane | - | Before cure |
| Work life | 60 | min | At room temperature |
| Sag resistance | Approximately 30 | sec | After mixing |
After-processing / final-state properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Overlap shear strength | 2500 | psi | Etched aluminum; tested at -40 deg C |
| Overlap shear strength | 2000 | psi | Etched aluminum; tested at 24 deg C |
| Overlap shear strength | 300 | psi | Etched aluminum; tested at 82 deg C |
| Overlap shear strength | 1200 | psi | Abraded and solvent-wiped steel; tested at 24 deg C |
| Handling-strength time | 7 | days | At room temperature |