3M EZ250150
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Extended 2 to 4 Minute Open Time
- Aluminum or Glass to Wood or Plastic
- Flexible Cured Adhesive Layer
Product Description
3M Scotch-Weld PUR Easy 250 Plastic Adhesive EZ250150 is a one-component, 100% solids moisture-curing polyurethane reactive adhesive for longer assembly windows on larger or more complex parts. Applied warm at 121 deg C, it provides an open time of 2 to 4 minutes and a set time of 30 to 150 seconds. Supported combinations include wood-to-wood, plastic-to-plastic, wood-to-plastic, aluminum-to-wood or plastic, and glass-to-wood or plastic. A typical elongation at break of 700% after seven days at 23 deg C indicates a flexible cured adhesive layer that can deform before breaking. Moisture access is required, so metal-to-metal, glass-to-glass, and metal-to-glass bonds are excluded.
Key features
- Longer assembly window: An open time of 2 to 4 minutes and a set time of 30 to 150 seconds support larger or more complex assemblies.
- Supported substrate combinations: Bonds wood and plastics and joins aluminum or glass to wood or plastic while preserving moisture-access limits.
- Flexible cured adhesive layer: A typical 700% elongation at break indicates a cured layer that can deform before breaking rather than acting as a rigid bondline.
Applications
Applications include larger or more complex wood, plastic, aluminum-to-wood or plastic, and glass-to-wood or plastic assemblies that benefit from the longer open and set window.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Mechanical Properties
Additional Information
As-supplied / before-processing properties
Open and handling times are approximate and depend on adhesive temperature and application conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color, solid | White to off-white | As supplied | |
| Viscosity | 9,000 | cP | 121 deg C; Brookfield Thermosel, spindle No. 27 |
| Density, molten | 9.1 | lb/gal | Typical |
| Solids content | 100 | % | Typical |
| Application temperature | 121 | deg C | 250 deg F |
| Open time | 2 to 4 | minutes | Product feature range |
| Set time | 30 to 150 | seconds | Product feature range |