3M SJ5816
Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide
Main features
- Die-Cut Protective Conversion
- Skid-Resistant Polyurethane Cushioning
- High-Tack PSA Installation
Product Description
3M Bumpon Resilient Rollstock SJ5816 is a black, self-adhesive solid polyurethane rollstock for conversion into die-cut feet, stops, spacers, and cushioning parts. The 1.6 mm sheet combines Shore M 72 polyurethane with an R-30 natural-rubber pressure-sensitive adhesive and PET release liner. Its resilient, skid-resistant surface is used to reduce vibration and noise, cushion components, and protect finished surfaces from scratching or marring. The roll format supports custom shapes and sizes, while the pressure-sensitive backing simplifies placement after die cutting. SJ5816 is intended primarily for interior applications; protected outdoor use may show discoloration or chalking.
Key features
- Die-cut rollstock conversion: Converts into custom feet, stops, spacers, gaskets, and protective shapes.
- Skid-resistant cushioning: Solid polyurethane provides grip, cushioning, and vibration or noise damping in compact assemblies.
- Natural-rubber PSA mounting: R-30 adhesive provides high initial tack for pressure-sensitive placement after conversion.
Applications
Applications include die-cut protective feet, stops, spacers, gaskets, anti-rattle parts, cushioning elements, and non-scratch surface protection.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Mechanical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Construction and physical values apply to SJ5816 or the SJ5800 series as indicated.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Color | Black | SJ5816 | |
| Elastomer | Solid polyurethane | SJ5800 series construction | |
| Adhesive | R-30 natural rubber | Pressure-sensitive adhesive | |
| Surface finish | Matte | Polyurethane surface | |
| Nominal thickness | 1.6 | mm | ASTM D3767 Procedure A; measured without liner |
| Hardness | 72 | Shore M | ASTM D2240 |
After-processing / final-state properties
Performance values are typical for SJ5816 or the SJ5800 series under the stated test conditions.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Kinetic coefficient of friction | >1 | ASTM D1894; stainless steel and glass | |
| Kinetic coefficient of friction | 0.8 to 1.4 | ASTM D1894; Formica laminate and wood | |
| 90 deg peel adhesion | 25 | oz/0.5 in | Polypropylene, polystyrene, or ABS; 72 h dwell; 3M TM-2011 |
| 90 deg peel adhesion | 22 | oz/0.5 in | Stainless steel or aluminum; 72 h dwell; 3M TM-2011 |
| Recommended maximum load | 100 | psi | 21 to 49 deg C; SJ5800 series |
| Service temperature | -34 to 66 | deg C | 107 deg C intermittent exposure |