ABchimie 6025UV LED Soft Thixotropic Resin
Harmonization Code : 3906909090 | Acrylic polymers in primary form Others>Others
Main features
- One component
- UV LED Cure
- Shock Absorbing
Product Description
ABChimie® 6025UV LED is a soft, transparent resin coating designed to provide mechanical and environmental protection to electronic components and assemblies. Its thixotropic quality allows for controlled application with high thicknesses (up to 4mm) without sagging. The resin is soft, which allows it to absorb shock easily. These qualities make it ideal for encapsulation or localized protection in applications where shock absorption is required.
ABChimie® 6025UV LED is acrylic-based and has excellent adhesion to many substrates, including flexible ones like plastics. One of its advantages is that it cures rapidly under UV LED light (395 nm), has zero VOCs, and can be applied to high-speed manufacturing processes to increase productivity. ABChimmie 6025UV LED is in full compliance with REACH and RoHS regulations.
Product Key Features
- Transparent, thixotropic UV-curing resin
- Shock absorbing
- Allows for thick, controlled application without sagging
- Fast UV cure for high-sp
- Solvent-free formulation (no VOCs)
- LED Curing for worker / environmental safety
Applications
- Encapsulation of electronic components requiring high volumes, localized protection, and a thick coating
- Sensors on PCBs, wire-bonded chips, and reinforcement of solder joints.
- Can be used to seal plastic casings on PCBs.
- Ideal for applications that might be exposed to impacts, drops, or vibrations.
- Printed circuit assemblies.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Mechanical Properties
Additional Information
Frequently Asked Questions About ABChimie® 6025 UV LED
What are typical applications for ABChimie® 6025 UV LED?
ABChimie® 6025 UV led is an LED UV-curable resin designed to protect printed circuit board assemblies (PCBs) and components in demanding manufacturing environments, including:
- Automotive electronics (e.g., control units, sensors)
- Industrial automation (e.g., motor drives, PLCs)
- Consumer electronics (e.g., smart devices, wearables)
- Other high-reliability electronic assemblies
Why choose ABChimie® 6025 UV LED?
ABChimie® 6025 UV LED delivers rapid LED UV curing, excellent electrical insulation, thixotropic application properties, and strong adhesion to flexible substrates. It supports high-throughput manufacturing while providing durable protection for sensitive components.
What is the recommended curing method for ABChimie® 6025 UV LED?
ABChimie® 6025 UV LED is UV-curable and should be cured with a mercury lamp. The minimum UVA dose is 1000 mJ/cm² for a 1mm thickness. The mercury lamp-curable version is ABChimie® 6025 UV. Higher UVA doses do not negatively affect final properties.
Learn More About ABChimie® 6025 UV LED
ABChimie® 6025 UV LED is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable resin delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for applications in automotive electronics, industrial automation, consumer electronics, and other high-reliability assemblies.
Main Advantages of ABChimie 6025 UV LED
ABChimie® 6025 UV LED cures rapidly under UV light, enabling integration into both batch and inline production. The resin forms a durable, high-performance layer that protects assemblies while supporting high-throughput manufacturing.
ABChimie® 6025 UV LED cures to a Shore hardness of A60 , providing excellent mechanical protection. This hardness helps resist scratches, abrasion, and minor impacts, ensuring long-term stability of encapsulated components.
ABChimie® 6025 UV LED is thixotropic: it maintains a stable, non-running consistency at rest but flows easily under shear during application. This ensures precise placement, minimal sagging, and uniform coverage before rapid UV curing.
ABChimie® 6025 UV LED bonds strongly to flexible substrates, including plastics and polymer-based PCBs. Its adhesion ensures reliable protection even on surfaces that bend or flex, ideal for wearables, flexible electronics, and lightweight assemblies.
How to Choose a Resin
Selecting the most suitable resin requires consideration of key factors:
- ✔ Norms & Compliance
- ✔ Environment / Exposure Conditions
- ✔ Repairability
- ✔ Electrical Performance
- ✔ Application Method
- ✔ Operating Temperature
Compliance You Can Trust ✅
ABChimie® 6025 UV LED meets stringent industry standards, ensuring reliability and regulatory adherence for OEMs and contract manufacturers:
- REACH Compliant
- RoHS 2011/65/EU Compliant
Curing Tip: ABChimie 6025 UV LED cures with UV rays. It is crucial to use the appropriate equipment, as well as the recommended settings, to achieve the best properties of the resin.
Ref. Leistung / ref power ln % over wavelength in nm
Ref. Leistung / ref power ln % over wavelength in nm
Key Curing Properties
LED
395 nm
3000 mJ/cm2
7200 mJ/cm2
Coating Thickness
1 mm
3 mm
Typical property values shown for reference only and should not be used as specifications.
Alternative to LED Lamp Curing of ABChimie 6025 UV LED
ABChimie 6025 UV LED is also available in the mercury lamp - version, which cures by mercury lamp.
ABChimie 6025 UV [Go to 6025 UV Product Page↗]
- Thixotropic resin
- Fluorescent under UV light
- Excellent adhesion to flexible substrates
- Immediate curing with UV LED exposure
Best suited for: High-speed process looking to use LED light for curing