ABchimie746E UV LED Soft UV Cure Conformal Coating
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- Excellent adhesion
- UV‑fluorescent for easy inspection
- Certified UL94 V‑0 and UL746E
Product Description
ABchimie 746E UV LED is a transparent, single‑component, LED‑curable conformal coating engineered to protect PCBs exposed to harsh environments. It features dual‑cure technology (UV LED + humidity) for complete crosslinking, including areas shadowed from UV LED exposure.
Its optimized formulation cures rapidly under UV LED light sources, enabling energy‑efficient, low‑temperature, high‑speed manufacturing. With low viscosity designed for precise application around 80 µm, ABchimie 746E UV LED is ideal for advanced selective coating processes.
Product Key Features
- Excellent adhesion in harsh climatic and environmental conditions
- UV‑fluorescent for easy inspection of coating uniformity
- Operating temperature range: –65°C to +150°C
- Safe solder‑through performance without toxic gas formation
- Certified UL94 V‑0 and UL746E (QMJU2‑E308681)
Applications
- High‑volume production lines requiring instant UV LED curing
- Complex assemblies with shadowed areas requiring dual‑cure reliability
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Electrical Properties
Thermal Properties
Additional Information
Frequently Asked Questions About ABChimie® 746E UV LED
What are typical applications for ABChimie® 746E UV LED?
ABChimie® 746E UV LED is a low viscosity UV-curable conformal coating designed to protect printed circuit board assemblies (PCBs) and components in demanding manufacturing environments, including:
- Automotive electronics (e.g., control units, sensors)
- Industrial automation (e.g., motor drives, PLCs)
- Consumer electronics (e.g., smart devices, wearables)
- Other high-reliability electronic assemblies
What safety precautions should I take?
Use ABChimie® 746E UV LED in a well-ventilated area, avoid skin and eye contact, and follow all Safety Data Sheet (SDS) guidelines. Keep away from open flames and sparks.
Can I adjust the viscosity?
ABChimie® 746E UV LED can be customized for variable viscosities. Contact our team for guidance.
Should I control the application environment?
ABChimie® 746E UV LED should be applied at a minimum temperature of 16°C and a minimum relative humidity of 50%. The relative humidity of at least 50% is recommended for the secondary polymerization. Before applying, the PCB must be clean, dry, and free of moisture. A stage in an oven at 80°C for 4 hours is usually sufficient.
Learn More About ABChimie® 746E UV LED
ABChimie® 746E UV LED is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable conformal coating delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for automotive, industrial, consumer, and high-reliability assemblies. It also contains a UV tracer for easy inspection.
Main Advantages of ABChimie 746E UV LED
ABChimie® 746E UV LED cures through a dual mechanism: UV exposure initiates rapid surface curing, while moisture ensures complete curing throughout the coating.
Provides excellent mechanical protection, resisting scratches, abrasion, and minor impacts to ensure long-term component stability.
Can be soldered through without generating highly toxic gases, maintaining coating integrity.
Provides strong adhesion in harsh conditions, resisting moisture, chemicals, and temperature changes.
How to Choose a Conformal Coating
- ✔ Norms & Compliance
- ✔ Environment / Exposure Conditions
- ✔ Repairability
- ✔ Electrical Performance
- ✔ Application Method
- ✔ Operating Temperature
Compliance You Can Trust ✅
- REACH Compliant
- RoHS 2011/65/EU Compliant
UL94 V0
UL746E (QMJU2-E308681)
Curing Tip: ABChimie 746E UV LED cures with UV rays. Use the recommended equipment and settings to achieve optimal properties.
Ref. Leistung / ref power ln % over wavelength in nm

Key Curing Properties
LED
395 nm
3000 mJ/cm2
Coating Thickness
100 μm
Minimum UVA Power
500 mW/cm2
Typical property values shown for reference only and should not be used as specifications.
How to Optimise for the Best Results
PCBs must be completely dry and thoroughly clean, with no dust, grease, wax, or other contaminants. All flux residues must be removed to prevent corrosion or malfunctions.
For cleaning equipment or removing uncured ABChimie 746E UV or UV LED varnish, use SND or ABclean solvent.
Use the correct UV equipment and recommended settings to achieve optimal properties. UV exposure plus moisture curing ensures complete polymerization.

Curing Mechanism: UV light creates the first cure, and after 7 days, the moisture from the environment completes the curing process.
How does Moisture Cure Work?
During UV curing, exposure to UV light activates the photoinitiators in the conformal coating, triggering rapid polymerization of the resin. This results in an immediate surface cure and fast development of handling strength. UV curing provides precise, on-demand curing in exposed areas, enabling high-throughput processing while maintaining coating uniformity.
ABChimie 746E UV and ABChimie 746E UV LED use the same dual curing mechanism to ensure complete curing, including in shadowed or hard-to-reach areas. Initial curing is achieved by UV exposure, while a secondary moisture-activated cure completes the process at ambient temperature. For full curing in shaded areas, a minimum relative humidity of 50% is required for at least 7 days.
ABChimie 746E UV LED is also available in the mercury lamp version, which cures with a mercury lamp.
ABChimie 746E UV [Go to 746E UV Product Page↗]
- Conformal Coating
- Fluorescent under UV light
- Excellent adhesion to flexible substrates
- Dual curing with UV light exposure and moisture curing
Best suited for: High-speed process using LED light for curing