ABchimie 80K UV LED High Viscosity Resin

Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium

ABchimie 80K UV LED High Viscosity Resin

Main features

  • Soft, flexible resin
  • Excellent adhesion
  • UL 94 V‑0 flammability rating

Product Description

ABchimie 80K UV LED is a soft, one‑component resin optimized for UV LED curing, providing rapid, energy‑efficient polymerization with low heat generation. It is designed for local protection and mechanical reinforcement, especially for tall or vibration‑sensitive components.

The resin supports high‑thickness applications up to 5 mm, offering robust humidity and thermal resistance. With strong adhesion to numerous substrates and no VOC, ABchimie 80K UV LED enables clean and efficient processing in modern electronic manufacturing environments.

Product Key Features

  • Soft, flexible resin for shock and vibration damping
  • Excellent adhesion on PCBs, plastics, and other substrates
  • High‑speed process suitable for modern LED‑equipped production lines
  • One‑component, ready‑to‑use formulation
  • UL 94 V‑0 flammability rating qualified (QMJU2‑E308681)

Applications

  • Local encapsulation using UV LED curing systems
Product Family

ABCHIMIE 80KUVLED

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Transparent liquid
Specific Gravity Specific Gravity
1.1
Physical Properties
Viscosity Viscosity
80000 mPa.s
Mechanical Properties
Durometer (Shore D) Durometer (Shore D)
15
Thermal Properties
Coefficient of Thermal Expansion (CTE), α1 Coefficient of Thermal Expansion (CTE), α1
50 ppm/°C
Coefficient of Thermal Expansion (CTE), α2 Coefficient of Thermal Expansion (CTE), α2
150 ppm/°C
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
-19 °C
Electrical Properties
Breakdown Voltage Breakdown Voltage
1500 V
Dielectric Strength Dielectric Strength
60 kV/mm

Additional Information

Curing Profile

Recommended settings for the best properties of the resin ABchimie80K UV LED (LED lamp 395 nm):

  • Minimum UVA2 dose : 3000mJ/cm2 (to a 1mm-thickness)

The UVA dose is a minimum dose recommended. The intensity depends on the lamp power and the lampe distance.

UVA dose may be increased by a longer exposure time. A higher dose of UV or an overexposure will not damaged the product. However a lower UVA dose can have a detrimental effect on product final properties therefore it is very important to ensure minimum recommended UVA dose is met with your curing system.

Leading Brands Trust in Our Products and Services