ABchimie836UV LED Soft Dual Cure Conformal Coating
Harmonization Code : 3208.20.90 | Paints and varnishes that are dispersed or dissolved in a non aqueous medium
Main features
- One Component
- Dual Cure (UV LED and Humidity)
- Excellent Moisture Resistance
Product Description
ABChimie® 836UV LED is a transparent urethane acrylate conformal coating designed to provide mechanical and environmental protection to electronic components and assemblies. It features dual-cure technology (UV and humidity), which allows for the complete crosslinking through the entire PCB, even in areas that may be covered by shadow. The coating also allows the PCB to be soldered through without producing toxic gases.
ABChimie 836UV LED exhibits excellent moisture resistance in humid environments (Log Ohm> 10.5, IPC CC 830, SIR per IPC TM 650 2.6.3.4), which makes it ideal for conformal coating applications. The ideal application method is selective coating. One of its advantages is that it cures rapidly under UV light, has zero VOCs, and can be applied to high-speed manufacturing processes to increase productivity. ABChimmie 836UV LED is in full compliance with REACH and RoHS regulations, and also has UL94 V0 and UL746E (QMJU2-E308681) certifications.
Product Key Features
- Transparent
- Dual Cure (UV + Humidity)
- Thin film thickness (30 - 130 microns)
- Excellent adhesion to PCBs
- Resists mold growtn
- Fast UV cure for high volume production
- Solvent-free formulation (no VOCs)
- Spray and Selective Coating (ideal) applications
- UL94 V0 and UL746e
Applications
- Conformal coating for Printed circuit assemblies.
- Protection for plastic casings or covers.
- Protection for optically clear applications ex. lenses.
Packaging
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Electrical Properties
Thermal Properties
Physical Properties
Additional Information
Frequently Asked Questions About ABChimie® 836 UV LED
What are typical applications for ABChimie® 836 UV LED?
ABChimie® 836 UV LED is a UV-curable conformal coating designed to protect printed circuit board assemblies (PCBs) and components in demanding manufacturing environments, including:
- Automotive electronics (e.g., control units, sensors)
- Industrial automation (e.g., motor drives, PLCs)
- Consumer electronics (e.g., smart devices, wearables)
- Other high-reliability electronic assemblies
What safety precautions should I take?
Use ABChimie® 836 UV LED in a well-ventilated area, avoid skin and eye contact, and follow all Safety Data Sheet (SDS) guidelines. Keep away from open flames and sparks.
Can I adjust the viscosity?
ABChimie® 836 UV LED can be customized for variable viscosities. Contact our team for guidance.
Should I control the application environment?
ABChimie® 836 UV LED should be applied at a minimum temperature of 16°C and a minimum relative humidity of 50%. The relative humidity of at least 50% is recommended for the secondary polymerization. Before applying, the PCB must be clean, dry, and free of moisture. A stage in an oven at 80°C for 4 hours is usually sufficient.
Learn More About ABChimie® 836 UV LED
ABChimie® 836 UV LED is a proven solution for engineers seeking fast, reliable protection of electronic assemblies in demanding manufacturing environments. This UV-curable conformal coating delivers rapid curing, excellent electrical insulation, and strong environmental resistance—ideal for automotive, industrial, consumer, and high-reliability assemblies.
Main Advantages of ABChimie 836 UV LED
ABChimie® 836 UV LED cures through a dual mechanism: UV exposure initiates rapid surface curing, while moisture ensures complete curing throughout the coating.
Provides excellent mechanical protection, resisting scratches, abrasion, and minor impacts to ensure long-term component stability.
Can be soldered through without generating highly toxic gases, maintaining coating integrity.
Provides strong adhesion in harsh conditions, resisting moisture, chemicals, and temperature changes.
How to Choose a Conformal Coating
- ✔ Norms & Compliance
- ✔ Environment / Exposure Conditions
- ✔ Repairability
- ✔ Electrical Performance
- ✔ Application Method
- ✔ Operating Temperature
Compliance You Can Trust ✅
- REACH Compliant
- RoHS 2011/65/EU Compliant
UL94 V0
UL746E (QMJU2-E308681)
Curing Tip: ABChimie 836 UV LED cures with UV rays. Use the recommended equipment and settings to achieve optimal properties.
Ref. Leistung / ref power ln % over wavelength in nm

Key Curing Properties
LED
395 nm
3000 mJ/cm2
Coating Thickness
100 μm
Minimum UVA Power
500 mW/cm2
Typical property values shown for reference only and should not be used as specifications.
How to Optimise for the Best Results
PCBs must be completely dry and thoroughly clean, with no dust, grease, wax, or other contaminants. All flux residues must be removed to prevent corrosion or malfunctions.
For cleaning equipment or removing uncured ABChimie836UV or UV LED varnish, use SND or ABclean solvent.
Use the correct UV equipment and recommended settings to achieve optimal properties. UV exposure plus moisture curing ensures complete polymerization.
Curing Mechanism: UV light creates the first cure; moisture completes the curing process over 7 days.
How does Moisture Cure Work?
Exposure to UV light activates photoinitiators, triggering rapid polymerization for surface cure. A secondary moisture-activated cure completes the process in shadowed areas over 7 days at ≥50% RH.
ABChimie 836 UV LED is also available in the mercury lamp version, which cures with a mercury lamp.
ABChimie 836 UV [Go to 836 UV Product Page↗]
- Conformal Coating
- Fluorescent under UV light
- Excellent adhesion to flexible substrates
- Dual curing with UV light exposure and moisture curing
Best suited for: High-speed process using LED light for curing