ABchimie ABclean Cleaning & Defluxing Solvent

Harmonization Code : 34021900 | Surface active agents

ABchimie ABclean Cleaning & Defluxing Solvent

Main features

  • Fast‑drying, non‑toxic cleaning solvent
  • Leaves no greasy or sticky residues after evaporation
  • High compatibility with a wide range of plastic materials

Product Description

ABchimie ABclean is a fast‑drying, non‑toxic solvent specially formulated for cleaning, defluxing, and degreasing electrical and electronic equipment. It is also highly effective for stripping conformal coatings from printed circuit boards. ABclean is 100% ozone‑friendly and offers excellent compatibility with a wide range of plastic materials, making it suitable for diverse maintenance and manufacturing environments.

ABclean dissolves acrylic and silicone varnishes quickly, providing efficient coating removal with minimal effort. Its rapid evaporation rate enhances cleaning performance, leaving surfaces clean, dry, and residue‑free. ABclean is part of ABchimie’s broad line of cleaning solutions, which includes both slow‑ and fast‑drying solvents and water‑based cleaners.

Product Key Features

  • Quickly dissolves acrylic and silicone conformal coatings
  • Fast‑drying, non‑toxic cleaning solvent
  • CFC-free and ozone-friendly
  • Excellent removal of oils, greases, flux residues, and coatings from PCBs
  • High compatibility with a wide range of plastic materials
  • Effective for both cleaning and stripping applications

Applications

Product Family

ABCHIMIE ABCLEAN

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Specific Gravity Specific Gravity
0.86
Thermal Properties
Flash Point Flash Point
12 °C

Leading Brands Trust in Our Products and Services