ABchimie NDD Cleaner, Degreaser & Flux Remover

Harmonization Code : 340290 | Organic surface active agents (other than soap), surface-active preparations, washing preparations (including auxiliary washing preparations

ABchimie NDD Cleaner, Degreaser & Flux Remover

Main features

  • Fast-drying
  • 100% ozone-friendly
  • Broad material compatibility

Product Description

ABchimie NDD is a fast‑drying, high‑purity solvent cleaner for quick and efficient removal of flux residues after soldering. NDD delivers superior cleaning performance on printed circuit boards and electronic assemblies while remaining safe for a wide range of materials. ABchimie NDD evaporates rapidly, leaving surfaces clean, dry, and free from residue.

Product Key Features

  • Fast‑drying solvent designed for post‑solder cleaning
  • 100% ozone‑friendly formulation with zero Ozone Depletion Potential (ODP)
  • Highly effective at removing greases, oils, flux residues, and acrylic conformal coatings
  • Leaves a perfectly clean, residue‑free surface—unlike conventional solvents that may leave greasy deposits
  • Broad material compatibility

Applications

Product Family

ABCHIMIE NDD

1. Select Package Type
Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

Product availability
EU Shipping in 8 weeks
Packaging
Please select Package Type.
TDS, SDS & Technical Documents

Technical Specifications

General Properties
Evaporation Rate Evaporation Rate
16
Specific Gravity Specific Gravity
0.79
Thermal Properties
Flash Point Flash Point
0 °C

Additional Information

Instructions for Use

ABchimie NDD contains flammable solvents so do not spray onto live electrical equipment or other sources of ignition. Immerse surface to be cleaned or spray onto surface to excess and allow to evaporate. A brush can be used to remove any stubborn deposits. For use for large scale production.