LOCTITE ABLESTIK 2112
Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm
Main features
- Critical Electronics/Aerospace Bonding
- Non-Sag PCB Component Staking
- Electrical Insulation and Environmental Resistance
Product Description
LOCTITE ABLESTIK 2112 BIPAX is a two-component, thixotropic, non-conductive epoxy adhesive supplied as a milky, translucent resin and hardener at a 100:22 mix ratio in a BIPAX mixing-dispenser package. This solvent-free system cures at room temperature over 24 hours or faster at 65°C, and supports continuous service from -60°C to 125°C. It is recommended for critical electronic, aerospace, and industrial bonding, laminating, and reinforcing applications, including staking components to printed circuit boards for enhanced mechanical rigidity. The non-sag rheology supports precise application, and the cured adhesive offers good chemical resistance, good electrical insulation, and environmental resistance across metals, glass, ceramics, wood, and plastics.
Key features
- Non-sag, thixotropic rheology: Supports precise application and PCB component staking without slumping.
- Good electrical insulation: Non-conductive with a dielectric strength of 410 volts/mil.
- Electronics and aerospace grade: Recommended for critical electronic, aerospace, and industrial bonding applications.
Applications / Suitable for: Critical electronic, aerospace, and industrial bonding, laminating, and reinforcing, including staking components to printed circuit boards.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Physical Properties
Thermal Properties
Electrical Properties
Additional Information
As-supplied / before-processing properties
Typical properties of the uncured, mixed material prior to cure.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Mix ratio (Resin : Hardener) | 100 : 22 | by weight | — |
| Viscosity, mixed | 60,000 | mPa·s (cP) | Brookfield RV #7, 10 rpm |
| Thixotropic index | 6.5 | — | 1/10 rpm ratio |
| Specific gravity, mixed | 1.2 | — | Mixed material |
| Pot life | 30 | minutes | @ 25°C, mixed |
As-supplied / before-processing properties
Typical properties of the uncured, mixed material prior to cure.
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Mix ratio (Resin : Hardener) | 100 : 22 | by weight | — |
| Viscosity, mixed | 60,000 | mPa·s (cP) | Brookfield RV #7, 10 rpm |
| Thixotropic index | 6.5 | — | 1/10 rpm ratio |
| Specific gravity, mixed | 1.2 | — | Mixed material |
| Pot life | 30 | minutes | @ 25°C, mixed |