ABLESTIK 216C03

Harmonization Code : 3214.10.00 | Putty and other mastics | Resin cements, caulking compounds and other mastics

ABLESTIK 216C03

Main features

  • Equal-Weight Mix Control
  • Ambient or Accelerated Cure
  • Flexible Non-Conductive Bonding

Product Description

LOCTITE ABLESTIK 216C03 is a two-part amber epoxy adhesive for general-purpose, electrically non-conductive bonding of plastic parts. The 100:100 resin-to-hardener ratio by weight simplifies equal-part preparation, while the mixed adhesive has a typical viscosity of 16,000 mPa s at 25 deg C. It can cure for 24 hours at 25 deg C or one hour at 65 deg C, allowing ambient or accelerated assembly schedules. The flexible, thixotropic formulation bonds nylon, PVC, polyethylene, acrylic, Lexan polycarbonate, polypropylene, Kapton polyimide film, and other thermoplastics. Cured aluminum lap-shear strength varies with the selected cure schedule.

Key features

  • Equal-weight mixing: A 100:100 resin-to-hardener ratio simplifies batch preparation and visual mix control.
  • Ambient or accelerated cure: Cures in 24 hours at 25 deg C or one hour at 65 deg C.
  • Flexible non-conductive bonding: Combines electrical isolation with a flexible epoxy bond for plastic-part assembly.

Applications

Applications include general-purpose assembly bonding of nylon, PVC, polyethylene, acrylic, Lexan, polypropylene, Kapton, and other thermoplastic parts.

Product Family

ABLESTIK 216C03

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Appearance Appearance
Amber
Component System Component System
Two (Resin / Hardener)
Mix Ratio Mix Ratio
100 : 100
Specific Gravity Specific Gravity
1.02
Thermal Properties
Glass Transition Temperature (Tg) Glass Transition Temperature (Tg)
18.0 °C

Additional Information

Technical properties

As-supplied / before-processing properties

The table separates mixed-material properties and recommended processing schedules from cured results.

PropertyValueUnitMethod / condition
AppearanceAmberMixed system
Mix ratio, resin:hardener100:100by weightTwo-part system
Mixed viscosity16,000mPa sBrookfield LV, spindle 4 at 12 rpm and 25 deg C
Ambient cure schedule24hours25 deg C
Heat cure schedule1hour65 deg C
Technical properties

After-processing / final-state properties

Cured values are typical and remain tied to the stated cure schedule and substrate.

PropertyValueUnitMethod / condition
Shore A hardness901 h at 65 deg C or 24 h at 25 deg C cure
Glass transition temperature18.0deg CDSC
Cured specific gravity1.02Typical cured material
Aluminum lap shear strength10.3N/mm^21 h at 65 deg C cure
Aluminum lap shear strength7.2N/mm^224 h at 25 deg C cure