LOCTITE ABLESTIK 563K
Harmonization Code : 3920.99.28.90 | Other plates, sheets, film, foil and strip, of plastics, non-cellular and not reinforced, laminated, supported or similarly combined with other materials ; Of other plastics ; Other; Other
Main features
- Good heat transfer
- Low squeeze out
- Thermally conductive
Product Description
LOCTITE ABLESTIK 563K epoxy adhesive film is suitable for bonding "hot" devices onto heat sinks where electrical insulation and good heat transfer are required. It exhibits low squeeze out during bonding. This product provides high strength over a wider temperature range than is normally associated with flexible films.
LOCTITE ABLESTIK 563K is a thermally conductive film with good heat transfer which manages to achieve a thin bondline with uniform bondline control. It comes without a carrier and is typically available in 50um and 75um microns.
Cure Schedule
- 30 minutes @ 150°C
- 2 hours @ 125°C
Packaging
Technical Specifications
General Properties
Thermal Properties
Additional Information
Outgassing
NASA Outgassing:
- TML, % 0.44
- CVCM, % 0.04