LOCTITE ABLESTIK 6202C-X
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Lage die sizes
- Low flow (less than 150μm)
- Low moisture uptake
Product Description
LOCTITE ABLESTIK 6202C-X B-stageable adhesive is ideal for laminate-based packages where tolerance and bleed need to be minimized. This low modulus adhesive is recommended for large die sizes.
LOCTITE ABLESTIK 6202C-X is a hybrid, silica filled material with low moisture uptake, low flow, low warpage, low modulus and long work life. It can be stencil printed and is usually used on laminates for chip scale packages.
Cure Schedule
- 30 minutes ramp from 30 to 90ºC, hold 60 minutes plus
- 30 minutes ramp to 175ºC, hold 60 minutes in vented magazine in an oven with good air flow
Packaging
Please select Package Type and Package Size.
Technical Specifications
General Properties
Work life @25°C
Work life @25°C
168 hours
Thermal Properties
Glass Transition Temperature (Tg)
Glass Transition Temperature (Tg)
40 °C
Physical Properties
Thixotropic index
Thixotropic index
2.5
Viscosity
Viscosity
30,000 mPa.s