LOCTITE ABLESTIK 84-1LMIS
Harmonization Code : 3506.91.90.99 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg ; Adhesives based on polymers of headings 3901 to 3913 or on rubber; Other ; Other
Main features
- Long work life
- Solvent free
- Electrically conductive
Product Description
LOCTITE ABLESTIK 84-1LMIS epoxy adhesive is designed for semiconductor packaging applications. This adhesive is ideal for application by dispensing or stamping.
LOCTITE ABLESTIK 84-1LMIS is a silver coloured, electrically conductive solvent free adhesive with a long work life, typically used in leadframe die attach applications.
Cure Schedule
- 1 hour @ 175°C
- 30 minutes @ 200°C