LOCTITE ABLESTIK 84-3LV
Harmonization Code : 3506.10.00.00 | Prepared glues and other prepared adhesives, not elsewhere specified or included; products suitable for use as glues or adhesives, put up for retail sale as glues or adhesives, not exceeding a net weight of 1 kg
Main features
- Solvent-free
- Long work life
- One component
Product Description
LOCTITE ABLESTIK 84-3LV adhesive is designed for die attach applications. It is a non conductive, solvent free material that is used as an electrically insulating adhesive.
LOCTITE ABLESTIK 84-3LV is a Low Viscosity version of LOCTITE ABLESTIK 84-3. It can be applied by stamping or syringe dispensing.
Cure Schedule
- 1 hour @ 150°C
- 2 hours @ 125°C
Technical Specifications
General Properties
Work life @25°C
Work life @25°C
336 hours
Thermal Properties
Glass Transition Temperature (Tg)
Glass Transition Temperature (Tg)
66 °C
Thermal Conductivity
Thermal Conductivity
0.5 W/m.K
Weight Loss @ 300°C
Weight Loss @ 300°C
0.12 %
Physical Properties
Thixotropic index
Thixotropic index
1.6
Viscosity
Viscosity
12,500 mPa.s