ABLESTIK GA 47-2LV
Harmonization Code : 5906100000 | Adhesive tape of a width not exceeding 20cm
Main features
- Gyro-Flotation-Fluid-Compatible Instrument Bonding
- 25 ppm/deg C Linear Thermal Expansion
- 2-Hour 95 deg C Cure
Product Description
LOCTITE® ABLESTIK GA 47-2LV is a green, low-viscosity, heat-cured epoxy instrument adhesive. It is documented as compatible with conventional gyro flotation fluids and has a coefficient of thermal expansion that approximates aluminum within a normal temperature range. The material provides a typical viscosity of 50,000 mPa·s, a 30-minute work life at 25°C, and guideline cure options of 2 hours at 95°C or 4 hours at 75°C. Cured aluminum-to-aluminum lap shear strength is reported as 13.8 N/mm². :contentReference[oaicite:0]{index=0}
Key features
- Gyro-fluid compatibility: Documented compatibility with conventional gyro flotation fluids supports evaluation for applicable instrument assemblies. :contentReference[oaicite:1]{index=1}
- Aluminum-matched thermal expansion: The coefficient of thermal expansion approximates that of aluminum within a normal temperature range. :contentReference[oaicite:2]{index=2}
- Heat-cure flexibility: Guideline cure schedules include 2 hours at 95°C or 4 hours at 75°C. :contentReference[oaicite:3]{index=3}
Applications / Suitable for
- Instrument bonding applications
- Assemblies involving conventional gyro flotation fluids
- Bonding aluminum components under the documented cure conditions
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Thermal Properties
Additional Information
As-supplied / before-processing properties
Typical properties and processing characteristics of the adhesive before cure. :contentReference[oaicite:4]{index=4}
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Technology | Epoxy | — | As supplied |
| Appearance | Green liquid or paste | — | TDS appearance and SDS physical state |
| Viscosity | 50,000 | mPa·s (cP) | Test method and temperature not stated |
| Specific gravity | 2.1 | — | As supplied |
| Work life | 30 | minutes | At 25°C |
| Shelf life | 365 | days | At -40°C |
| Cure schedule | 2 hours or 4 hours | — | 2 hours at 95°C or 4 hours at 75°C; guideline recommendations |
After-processing / final-state properties
Typical properties and performance data for the cured adhesive. Values are reference data rather than product specifications. :contentReference[oaicite:5]{index=5}
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Hardness | 90 | Shore D | Test method and cure condition not stated |
| Glass-transition temperature | 95.0 | °C | Method and cure condition not stated |
| Coefficient of linear thermal expansion — below Tg | 25 | ppm/°C | Below Tg; method and cure condition not stated |
| Lap shear strength — aluminum to aluminum | 13.8 (2,000) | N/mm² (psi) | Substrate preparation, bondline, cure condition, test method, and test temperature not stated |