NanoProof 2.1 PCB Waterproofing Surface Treatment

Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated

NanoProof 2.1 PCB Waterproofing Surface Treatment

Main features

  • Hydrophobic treatment
  • 30-50 μm thickness
  • IPX7, IPX8

Product Description

NanoProof 2.1 is a surface treatment designed to impart hydrophobicity and reduced friction to circuit boards and electronic components. It is a simple, one-step process that provides a basic protective film for liquids. 

NanoProof 2.1 is a PFAS free, easy to use, and the dried film is nonconductive. The treatment can adhere to a broad range of substrates and contains a UV tracer. This product also requires no cure and can be applied through various methods including dispense and dip. 

 

Advantages of Aculon's NanoProof 2.1

  • More forgiving during application
  • 30-50 μm thickness
  • No cure required
  • Deformable (gel like) coating so needs to be handled with care
  • Contains UV tracer
  • RoHS and REACH compliant
  • PFAS Free

 


Utilization of multiple options
Please note that many customers have found significant success utilizing two or more of the available NanoProof® technologies successfully. Often times the most sensitive components benefit from the most robust NanoProof® technology (5.1) while the remaining components can be coated with the less robust coatings to benefit from their electrical push-through capability, flexible nature, and lower costs!

 

Detection/Inspection

All NanoProof products contain a UV Tracer which is visible under 365nm wavelength UV light (Detectable by both the human eye and automated detection systems). Please note that soldermasks and other substrate materials containing a UV tracer may make accurate detection of NanoProof difficult.

Product Family

ACULON NanoProof 2.1

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

General Properties
Color Color
Clear
Solids Solids
20 %
Specific Gravity Specific Gravity
0.79
Total Thickness Total Thickness
30-50 μm
Thermal Properties
Boiling Point Boiling Point
101 °C
Flash Point Flash Point
-4 °C
Electrical Properties
Volume Resistivity Volume Resistivity
1.93 *10^12 Ohms⋅cm
Physical Properties
Viscosity Viscosity
5000 mPa.s

Additional Information

How to apply NanoProof 2.1

STEP 1 ⇨ CLEAN

STEP 2 ⇨ TREAT

STEP 3 ⇨ DRY

Parts must be sufficiently clean before treatment for proper bonding and effective application. This can be accomplished by first degreasing the surface with solvents/rinsing with IPA.

Dip - Fully immerse the part in the treatment solution and withdraw at 1-5 mm/second (faster withdraw rate increases coating thickness).

 

To dry, the part should be placed at room temperature until the solvent is evaporated. Depending on thickness, parts should be fully cured in 60 minutes.

 

 

Dispense - Dispense the treatment over the surface, applying enough to coat the entire surface. Allow excess material to drain.

 

 

Application Tips

  • In some cases, Kyzen cleaners like Ionox I3s416 or Cybersolv 141-R may be appropriate for removing surface contamination.
  • For dip applications, dip containers should be stainless steel, glass, or aluminum. Plastic containers are likely to contaminate the solution.
  • Use a microfiber cloth to wipe after cleaning.
  • Coat the substrate as soon as possible after cleaning to prevent recontamination.
  • Cure temperatures and conditions should be optimized based on substrate and durability requirements.
  • Expect no mask to be compatible
  • Methylcyclohexane can be used as a diluent 

 

 

Chemical Compatibility
Recommendation for tubing and plastics via application equipment
Compatible with: SS Nozzles/Dispensers, Polyethylene terephthalate (PET), Polytetrafluoroethylene (PTFE), 
Incompatible with: HDPE, LDPE, Polyurethane, PVC, Tygon, Noryl, ABS, PP, Polyphenol
ethylene ether, silicone, neoprene, EPM, and natural rubber

 

 