Aculon Nanoproof 3-001X
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated
Main features
- 0.1% Fluoroacrylate Solids
- 1 um Thickness
- 3M Novec 1720 replacement
Product Description
Aculon Nanoproof 3-001X is a highly effective electronic coating series designed to provide superior protection against moisture, chemicals, and corrosion for a wide range of electronic applications. With the discontinuation of the popular 3M Novec product line, the Aculon Nanoproof 3.0 series offers a readily available and accessible alternative for industries that require robust protection for their electronic devices.
Aculon Nanoproof 3-001X with 0.1% Fluoroacrylate solids, forms a thin, transparent layer that provides excellent anti-wetting and anti-stiction properties, protecting LED devices from harmful elements. With this amount of solids, it manages to reach a coating thickness of less than 1um. The coating also offers electrical insulation properties, reducing the risk of electrical shorts and failures of PCBs and Electrical components.
The Aculon Nanoproof 3.0 series comes in different grades, with Aculon Nanoproof 3-001X allowing such a thin coating that is adirect alternative to 3M 1720 Novec products It is ideal for use in harsh environments, making it a popular choice in industries such as automotive, aerospace, and defense. Aculon Nanoproof 3-001X is easy to apply, and its transparent coating ensures that it does not interfere with the aesthetics or functionality of electronic devices. It is suitable for use on a variety of electronic applications, including printed circuit boards, sensors, switches, and connectors.
Applications:
- Moisture, chemical, and corrosion protection for printed circuit boards and electrical components
- Anti-wetting and anti-stiction in many diverse applications
Packaging
Technical Specifications
General Properties
Thermal Properties
Other Properties
Additional Information
Thickness depends on the amount of Solids. The higher the amount of solids, the thicker the coating after the solvent evaporates.
Aculon Nanoproof 3-001X vs 3M Novec 1720
| 3M Novec 1720 | Aculon Nanoproof 3-001X | |
| Solids | Fluoroacrylate 0.1% | Fluoroacrylate 0.1% |
| Solvent | 7100DL | 3 Series Extender |
| Appearance | Clear | Clear |
| Density | 1.5 g/ml | 1.5 g/ml |
| Viscosity | <20 cP | <20 cP |
| Boiling point | 61°C | 56-61°C |
| Environmental | Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine | Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine |
| Shelf life | 2 years | 2 years |
| Thickness | <1 um | <1 um |
| Tg | -110°C | 95°C |
| Thermal Stability of dry film | 200°C om air >3h | In process |
| Contact angles | WCA/OCA: 105°/65° | WCA/OCA: 120°/80° |
| Refractive Index | 1.39 | 1.376 |
| Solder through repairability | Yes | Yes |
| Cure | 135°C for 15 minutes | None |
| Application | Anti stiction, Chemical protection, Corrosion protection, Moisture protection | Anti stiction, Chemical protection, Corrosion protection, Moisture protection |
| Application location | LED | LED |