Aculon Nanoproof 3-10
Harmonization Code : 2901.10.00.00 | Acyclic hydrocarbons; Saturated
Main features
- 10% Fluoroacrylate Solids
- 0.25 - 6 um Thickness
- 3M Novec 1710 replacement
Product Description
Nanoproof 3-10 is a highly effective electronic coating series designed to provide superior protection against moisture, chemicals, and corrosion for a wide range of electronic applications. With the discontinuation of the popular 3M Novec product line, the Aculon Nanoproof 3.0 series offers a readily available and accessible alternative for industries that require robust protection for their electronic devices.
Nanoproof 3-10 with 10% Fluoroacrylate solids, forms a thin, transparent layer that provides excellent anti-wetting and anti-stiction properties, protecting electronic devices from harmful elements. With this amount of solids, it manages to reach a coating thickness of 0.25 - 6um. The coating also offers electrical insulation properties (3600V/mil Dielectric Strength), reducing the risk of electrical shorts and failures of PCBs and Electrical components.
The Aculon Nanoproof 3.0 series comes in different grades, with Aculon Nanoproof 3-10 offering similar performance and chemical properties to the 3M Novec 1710 products. It is ideal for use in harsh environments, making it a popular choice in industries such as automotive, aerospace, and defense. Aculon Nanoproof 3-10 is easy to apply, and its transparent coating ensures that it does not interfere with the aesthetics or functionality of electronic devices. It is suitable for use on a variety of electronic applications, including printed circuit boards, sensors, switches, and connectors.
Packaging
Technical Specifications
General Properties
Thermal Properties
Electrical Properties
Other Properties
Physical Properties
Additional Information
Thickness depends on the amount of Solids. The higher the amount of solids, the thicker the coating after the solvent evaporates.
Aculon Nanoproof 3-10 vs 3M Novec 1710
| 3M Novec 1710 | Aculon Nanoproof 3-10 | |
| Solids | Fluoroacrylate 10% | Fluoroacrylate 10% |
| Solvent | 7100DL | 347 |
| Appearance | Clear | Light Green |
| Density | 1.5 g/ml | 1.5 g/ml |
| Viscosity | 4.3 cP | <20 cP |
| Boiling point | 61°C | 56°C |
| Environmental | Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine | Non ozone depleting, low in toxocity, low in GWP, RoHS compliant and VOC exempt per US-EPA, contains no chlorine or bromine |
| Shelf life | 4 years | 2 years |
| Thickness | 0.1 - 1um | 0.25 - 6um |
| Tg | 44.5°C | 95°C |
| Thermal Stability of dry film | Can withstand 175°C for 24h and maintain repellency | Can withstand 175°C for 24h and maintain repellency |
| Contact angles | WCA/OCA: 105°/65° | WCA/OCA: 120°/80° |
| Refractive Index | 1.39 | 1.376 |
| Solder through repairability | Yes | Yes |
| Non-flammability | Meets UL 94 V-0 | Will meet UL 94 V-0 (Met via 5.5) |
| Dielectric Strength @ 35% RH | 2000 V/mil | 3600 V/mil |
| Cure | None | None |
| Application | Anti stiction, Chemical protection, Corrosion protection, Moisture protection | Anti stiction, Chemical protection, Corrosion protection, Moisture protection |
| Application location | PCB, Electrical components | PCB, Electrical components |