ALPHA 856
Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other
Main features
- Neutral Buffered Residue for Water Cleaning
- Fast-Recovering Foam for Production Coverage
- Defined Four-Hour Cleaning Window
Product Description
ALPHA 856 Liquid Soldering Flux is a neutral organic-acid, water-soluble liquid flux for wave soldering processes that use post-solder water cleaning. Its buffered activation system contains no free acid, and the post-solder residues are non-acidic. The low-smoking formulation is designed for foam application with a fine-bubble head that breaks quickly and recovers rapidly at production speed. During use, specific gravity at 25 deg C is maintained at 0.822 to 0.842 with ALPHA 425 thinner. Residues remain water soluble and should be thoroughly removed within four hours; hot DI-water rinsing at 50 to 60 deg C is specified for low ionic contamination before drying.
Key features
- Neutral buffered activation: Contains no free acid and produces non-acidic post-solder residues for controlled water-cleaned soldering processes.
- Fast-recovering foam coverage: A fine-bubble foam head breaks quickly and recovers rapidly to maintain coverage at production speed.
- Controlled water-cleaning window: Water-soluble residues should be removed within four hours, with a 50 to 60 deg C hot DI-water rinse used for low ionic contamination.
Applications
Used in water-cleaned wave soldering of electronic assemblies with foam flux application, controlled flux density, and prompt hot DI-water residue removal.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Colorless to pale yellow liquid | Typical | |
| Specific gravity | 0.832 +/- 0.005 | At 25 deg C (77 deg F) | |
| Non-volatiles | 15 | % | Typical |
| pH | 6.6 | 5% solution | |
| Halide as chloride | 2.33 +/- 0.23 | % | Typical |
| Flash point | 17 (62) | deg C (deg F) | T.C.C. |
| Shelf life | 720 | days | From date of manufacture |
| IPC classification | ORH1 | IPC J-STD-004 |