ALPHA 90IA
Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other
Main features
- High-Activity Difficult-Metal Soldering
- Low-Temperature Light-Gauge Processing
- Defined Acid-Wash Residue Removal
Product Description
ALPHA 90 Water Soluble Inorganic Acid Flux is a strong, highly active liquid flux for stainless steel and other difficult-to-solder metals. Its low activation temperature is suited to light-gauge materials where excessive heat can cause buckling or discoloration. Wetting agents promote rapid, uniform penetration into joint areas, while the active fluxing system reduces spattering. The flux is used for dip soldering and can be heated by torch, iron, oven, resistance, or induction methods. Post-solder residues are corrosive and must be removed promptly with a 1% hydrochloric acid solution followed by a water rinse. Typical specific gravity is 1.32 +/- 0.01 at 25 deg C.
Key features
- High-activity difficult-metal soldering: Designed for stainless steel and other difficult-to-solder metals that need strong inorganic-acid activation.
- Low-temperature activation: Supports light-gauge soldering where lower heat input helps limit buckling or discoloration.
- Defined residue removal: Corrosive post-solder residues are removed with a 1% hydrochloric acid wash followed by a water rinse.
Applications
Used for dip soldering of cans, hardware, and similar articles with torch, iron, oven, resistance, or induction heating across the listed difficult-to-solder metals.
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
| Property | Value | Unit | Method / condition |
|---|---|---|---|
| Appearance | Yellow to amber liquid | Typical | |
| Specific gravity | 1.32 +/- 0.01 | At 25 deg C (77 deg F) | |
| Weight per gallon | 11.0 | lb/gal | At 25 deg C (77 deg F) |
| Flash point | None | ||
| Shelf life | 1080 | days | From date of manufacture |