ALPHA K75I
Harmonization Code : 3404.90.00.00 | Artificial waxes and prepared waxes : Other
Main features
- ALPHA K75-I provides a high-purity isopropyl alcohol and de-ionized water extract solution designed for ionic cleanliness testing in compliance with MIL-P-28809.
- ALPHA K99-I provides a dedicated isopropyl-alcohol-based make-up solution for restoring K75-I to the desired alcohol/water ratio.
- The complementary K75-I/K99-I system supports regular alcohol-percentage adjustment to maintain the accuracy of the ionic test instrument procedure.
Product Description
ALPHA K75-I and K99-I Test Solutions are complementary solutions used for ionic cleanliness testing and control of the test-solution alcohol/water ratio. ALPHA K75-I Extract Test Solution consists of high-purity isopropyl alcohol and de-ionized water and is designed for cleanliness testing in compliance with MIL-P-28809. ALPHA K99-I Ratio Adjusting Solution is an isopropyl-alcohol-based make-up solution used with the Solution Control Nomogram to restore K75-I to the desired alcohol/water ratio as alcohol is lost through evaporation. Regular monitoring and adjustment with K99-I helps maintain the accuracy of the ionic test instrument procedure.
Key features
- Designed for ionic cleanliness testing: K75-I is formulated from high-purity isopropyl alcohol and de-ionized water for cleanliness testing in compliance with MIL-P-28809.
- Controlled test-solution ratio: K99-I is designed to restore K75-I to the desired alcohol/water ratio as alcohol is lost through evaporation.
- Supports test-procedure accuracy: Regular monitoring of alcohol percentage and adjustment with K99-I is used to maintain the ionic test instrument procedure.
Applications / Suitable for
- Ionic cleanliness testing using ALPHA K75-I Extract Test Solution
- Cleanliness testing in compliance with MIL-P-28809
- Adjustment of K75-I alcohol/water ratio using ALPHA K99-I
TDS, SDS & Technical Documents
Technical Specifications
General Properties
Additional Information
As-supplied / before-processing properties
Selected typical physical properties of ALPHA K75-I and ALPHA K99-I test solutions.
| Property | Value | Unit | Product / condition |
|---|---|---|---|
| Solution type | High-purity isopropyl alcohol and de-ionized water | - | ALPHA K75-I Extract Test Solution |
| Specific gravity | 0.855 | - | ALPHA K75-I, 77 °F |
| Density | 7.12 | lb/gal | ALPHA K75-I, 77 °F |
| Flash point | 70 | °F | ALPHA K75-I |
| Volatile | 100 | % | ALPHA K75-I |
| Solution type | Isopropyl-alcohol-based make-up solution | - | ALPHA K99-I Ratio Adjusting Solution |
| Specific gravity | 0.783 | - | ALPHA K99-I, 77 °F |
| Density | 6.52 | lb/gal | ALPHA K99-I, 77 °F |
| Flash point | 53 | °F | ALPHA K99-I |
| Volatile | 100 | % | ALPHA K99-I |