ALPHA RMA390

Harmonization Code : 3907.30.00.40 | Epoxy Mold Compounds containing by weight more than 70 % silicon dioxide

ALPHA RMA390

Main features

  • Wide reflow profile window supporting air and nitrogen reflow with straight-ramp or soak profiles up to 300 °C.
  • ROL0, halide-free rosin-based paste flux whose post-reflow residue is suitable to remain on the circuit board without cleaning.
  • Flexible application by screen printing, pin transfer, doctor blade, dip coating, or dispensing, with documented SIR and electromigration performance.

Product Description

ALPHA RMA-390-DH6 Paste Flux is a rosin-based paste flux designed for surface mount and other demanding electronic assembly applications. Its activator system is formulated to penetrate moderately tarnished surfaces, while the post-reflow residue is suitable to remain on the circuit board without cleaning. The flux supports air and nitrogen reflow using straight-ramp or soak profiles up to 300 °C and provides documented electrical reliability performance. ALPHA RMA-390-DH6 is classified ROL0 according to IPC J-STD-004 and can be applied by screen printing, pin transfer, doctor blade, dip coating, or dispensing.

Key features

  • Wide reflow profile window: Supports straight-ramp or soak profiles in both air and nitrogen reflow up to 300 °C.
  • No-clean residue capability: Post-reflow residue is suitable to remain on the circuit board without cleaning.
  • ROL0, halide-free formulation: Classified ROL0 per IPC J-STD-004, with halide-free status based on formulation.
  • Flexible application methods: Supports screen printing, pin transfer, doctor blade, dip coating, and dispensing.

Applications / Suitable for

  • Surface mount electronic assembly
  • High-density PWB assemblies
  • Applications involving moderately tarnished soldering surfaces
  • Screen printing, pin transfer, doctor blade, dip coating, and dispensing processes
Product Family

ALPHA RMA390

Catalog Product

Unlike other products we offer, the products listed on this page cannot currently be ordered directly from the website.

TDS, SDS & Technical Documents

Technical Specifications

No specifications available.

Additional Information

Technical properties

As-supplied / before-processing properties

Selected physical and chemical properties of ALPHA RMA-390-DH6 Paste Flux in its as-supplied state.

Property Value Unit Method / condition
Appearance Smooth, amber paste - As supplied
Viscosity 110 to 400 Poise Typical; Malcom Viscometer, 5 rpm at 25 °C
Fineness of grind <10 µm Physical property
Activity level ROL0 - IPC J-STD-004
Halide content Halide-free - Based on formulation
Technical properties

After-processing / final-state properties

Selected corrosion and electrical test results for ALPHA RMA-390-DH6 under the stated test conditions.

Property Result Method / condition
Copper mirror corrosion Pass IPC J-STD-004
SIR Pass, 2.5 x 1011 ohms Bellcore GR78-CORE; 96 hours at 35 °C/85% RH; pass ≥1 x 1011 ohms
Electromigration Pass, 2.2 x 1010 ohms Bellcore GR78-CORE; 500 hours at 65 °C/85% RH, 10 V; pass = final > initial/10
IPC SIR Pass, 1.1 x 109 ohms IPC J-STD-004A; 7 days at 85 °C/85% RH; pass >108 ohms
HP electrochemical migration Pass HP ECM; 28 days at 50 °C/90% RH, 10 V